Gussasphalt has been widely used as a surfacing material for long-span steel bridge decks. While most existing studies focus on the engineering properties of gussasphalt mixtures, this study aims to design gussasphalt mixtures using Trinidad Lake Asphalt (TLA) based on the mechanical performance of gussasphalt binders, mastics and mixtures. Three base asphalts (the styrene-butadienestyrene modified asphalt, the Pen 20/40 and Pen 60/80) and four dosages of TLA (20%, 30%, 40% and 50%) were used to prepare gussasphalt binders. The performance of Pen 20/40 with 30% TLA was found to be a qualified design according to the penetration, softening point and ductility of the gussasphalt binder and the dynamic shear properties of gussasphalt mortar. Afterward, optimum binder-aggregate ratio of 8.75% was obtained based on workability, high temperature performance, and low temperature performance. Lastly, the mechanical response of the gussasphalt mixture to dynamic loading was analysed using the dynamic frequency sweep test and triaxial repeated load permanent deformation test. The findings also indicated that the SBS modified asphalt binder may be not suitable as the base asphalt of gussasphalt. The cumulative strain level of gussasphalt mixture in triaxial loading linearly increased with respect to load stress, but exponentially increased with respect to testing temperature. (C) 2017 Elsevier Ltd. All rights reserved.
机译:Gussasphalt已被广泛用作大跨度钢桥面板的铺面材料。尽管大多数现有研究都集中在非马尾沥青混合物的工程特性上,但这项研究的目的是根据特马尼达沥青粘合剂,胶泥和混合物的机械性能,使用特立尼达湖沥青(TLA)设计非马蹄沥青混合物。使用三种基础沥青(苯乙烯-丁二烯-苯乙烯改性的沥青,Pen 20/40和Pen 60/80)和四剂TLA(20%,30%,40%和50%)来制备法沙沥青粘合剂。根据gussasphalt粘结剂的渗透性,软化点和延展性以及gussasphalt砂浆的动态剪切特性,发现Pen 20/40与30%TLA的性能是合格的设计。之后,基于可加工性,高温性能和低温性能,获得最佳的粘结剂-骨料比率为8.75%。最后,利用动态扫频试验和三轴反复载荷永久变形试验,分析了固式沥青混合料对动态载荷的力学响应。研究结果还表明,SBS改性沥青粘合剂可能不适合用作非天然沥青的基础沥青。在三轴载荷下,八卦石混合物的累积应变水平相对于载荷应力呈线性增加,但相对于测试温度则呈指数增长。 (C)2017 Elsevier Ltd.保留所有权利。

著录项

  • 来源
    《Construction and Building Materials》 |2017年第15期|131-141|共11页
  • 作者单位

    Southeast Univ, Intelligent Transport Syst Res Ctr, 35 Jinxianghe Rd, Nanjing 210096, Jiangsu, Peoples R China;

    Southeast Univ, Intelligent Transport Syst Res Ctr, 35 Jinxianghe Rd, Nanjing 210096, Jiangsu, Peoples R China;

    Monash Univ, Sch Engn, Malaysia Campus, Bandar Sunway 47500, Selangor, Malaysia;

    Southeast Univ, Intelligent Transport Syst Res Ctr, 35 Jinxianghe Rd, Nanjing 210096, Jiangsu, Peoples R China;

  • 收录信息 美国《科学引文索引》(SCI);美国《工程索引》(EI);
  • 原文格式 PDF
  • 正文语种 eng
  • 中图分类
  • 关键词

    Gussasphalt design; Trinidad Lake Asphalt; Binder-aggregate ratio; Workability; Mechanical response;

    机译:古萨沥青设计;千里达湖沥青;粘结剂-骨料比;可加工性;机械响应;