Mechanical strength and durability properties of concrete containing treated recycled concrete aggregates under different curing conditions

机译:含处理过的再生混凝土骨料的混凝土在不同养护条件下的机械强度和耐久性能

获取原文
获取原文并翻译 | 示例
           

摘要

This paper examines the mechanical and durability properties of concrete incorporated with treated recycled concrete aggregate (RCA) under different curing conditions. Three different curing regimes were applied, namely, continuous normal water curing (NW), initial water curing for 28 days before exposure to an open air environment (OA), and initial water curing for 28 days before exposure to seawater (SW). Two concrete mixes were produced by replacing 60% of the coarse aggregate using treated and untreated RCA with one control specimen (100% natural coarse aggregate) to examine the mechanical strength (compressive and flexural strength) and durability (water absorption, oxygen permeability, and also porosity) properties of the concrete. Meanwhile, the microstructure of these mixes was studied via scanning electron microscopy (SEM). The inclusion of untreated RCA generally reduces the mechanical strength and durability of the concrete regardless of the curing conditions. The compressive strength of the concrete containing untreated RCA is more detrimental in SW than in the other two curing conditions. Moreover, the concrete with RCA have poor intrinsic air permeability and porosity because their intrinsic porosity and effect are more significant when the curing is performed in OA than in the other curing conditions. Incorporating the treated RCA helps limit the reduction in the mechanical strength and durability of the concrete particularly under a prolonged curing period. (C) 2017 Elsevier Ltd. All rights reserved.
机译:本文研究了在不同养护条件下掺入经过处理的再生混凝土骨料(RCA)的混凝土的机械和耐久性能。应用了三种不同的固化方式,即连续正常水固化(NW),在暴露于露天环境(OA)之前先进行28天的初始水固化,以及在暴露于海水(SW)之前先进行28天的初始水固化。通过使用一个和未经处理的RCA将60%的粗骨料替换为一个对照样品(100%天然粗骨料)来生产两种混凝土混合物,以检查机械强度(抗压强度和抗弯强度)和耐久性(吸水率,透氧性和混凝土的孔隙率)。同时,通过扫描电子显微镜(SEM)研究了这些混合物的微观结构。不论固化条件如何,包含未处理的RCA通常都会降低混凝土的机械强度和耐久性。与其他两种固化条件相比,含未经处理的RCA的混凝土的抗压强度在SW中更有害。而且,具有RCA的混凝土具有固有的透气性和孔隙率差,这是因为当在OA中进行固化时,其固有的孔隙率和效果比在其他固化条件下更为显着。掺入处理过的RCA有助于限制混凝土的机械强度和耐久性的降低,特别是在延长固化时间的情况下。 (C)2017 Elsevier Ltd.保留所有权利。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号