This paper describes a laboratory procedure to study the sound absorption characteristics of porous asphalt pavement wearing course mix designs, and estimate their contributions to tire-pavement noise reduction. The effects of the following mixture properties were considered: percent porosity of mixture, degree of clogging occurred, and layer thickness. Four porosity levels of porous asphalt were studied: 12%, 16%, 20% and 25%. The mix design with 20% porosity was tested for the effects of clogging and specimen thickness respectively. A dense graded mix was included to serve as a reference for comparison. The effectiveness of the sound absorption and tire-pavement noise reducing capability of the mixtures were evaluated using the laboratory data and field measurements of trial sections. An approximate noise reduction calculation based on laboratory sound absorption measurements is proposed for comparison of different mix designs. The study found that changing the percent porosity from 25% to 12% caused some changes in the frequency characteristics of sound absorption, but made negligible changes in their contributions to tire-pavement noise reduction. On the other hand, clogging of the pores in the mixtures resulted in noticeable decreases in both the sound absorption coefficients and tire-pavement noise reductions. The analysis estimates that about 23-33% of the total tire-pavement noise reduction achieved by the porous asphalt mixtures can be attributed to their sound absorption capability. Finally, changing the thickness of the asphalt mixture tested from 63 mm to 200 mm had no significant effect on sound absorption and tire-pavement noise reduction. (C) 2017 Elsevier Ltd. All rights reserved.
机译:本文介绍了一种实验室程序,以研究多孔沥青路面穿着层配合料设计的吸声特性,并评估其对降低轮胎路面噪声的贡献。考虑以下混合物性质的影响:混合物的孔隙率百分比,发生堵塞的程度和层厚度。研究了多孔沥青的四个孔隙率水平:12%,16%,20%和25%。测试了孔隙率为20%的混合料设计对堵塞和试样厚度的影响。包括浓稠的渐变混合物,以作为比较的参考。使用实验室数据和试验区域的现场测量评估了混合物的吸声和轮胎路面降噪能力的有效性。提出了一种基于实验室吸声测量的近似降噪计算方法,用于比较不同的混合设计。研究发现,将孔隙率百分比从25%更改为12%会导致吸声频率特性发生一些变化,但对轮胎路面降噪的影响却可以忽略不计。另一方面,混合物中孔的堵塞导致吸声系数显着降低和轮胎路面噪声降低。分析估计,由多孔沥青混合物实现的轮胎路面总降噪量的约23-33%可以归因于其吸声能力。最后,将测试的沥青混合料的厚度从63 mm更改为200 mm对吸声和轮胎路面降噪没有明显影响。 (C)2017 Elsevier Ltd.保留所有权利。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号