首页> 外文期刊>Construction and Building Materials >Influence of recycled concrete and steel slag aggregates on warm-mix asphalt properties
【24h】

Influence of recycled concrete and steel slag aggregates on warm-mix asphalt properties

机译:再生混凝土和钢渣骨料对热拌沥青性能的影响

获取原文
获取原文并翻译 | 示例
       

摘要

This paper focuses on the comparison of the mechanical performance of three warm-mix asphalt (WMA) blends with recycled concrete aggregate (RCA) or electric arc furnace slag (EAFS) as substitutes of part of the aggregate. A conventional hot mix asphalt (HMA) and a WMA without by-products were used as references. The evaluation was carried out in a laboratory by means of testing specimens taken from experimental pavement sections built in real production, laying and compaction circumstances. Performance testing included wheel-tracking tests, four-point bending tests, and indirect tensile strength to assess water sensitivity. An organic wax and a chemical surfactant were applied to lower handling temperatures of the WMA under study. Apart from the HMA and the WMA used as references, the study evaluated the influence of introducing 60% of RCA or 30% of EAFS into the WMA blends as substitutes of the aggregate. The obtained results for the WMA with by-products tested allowed to conclude that the introduction of EAFS or RCA into the WMA blends increases Marshall stability and may increase or decrease resistance to rutting. Findings also showed that stiffness modulus is somewhat reduced and fatigue resistance does not change significantly. Additionally, water sensitivity is slightly reduced. Comparing these results with the performance observed elsewhere for WMA without by-products revealed that the addition of RCA or EAFS is satisfactory. The construction of experimental sections used conventional batch plant, paver and compactors without any noticeable technical problems. (C) 2018 Elsevier Ltd. All rights reserved.
机译:本文着重比较三种热拌沥青(WMA)掺混料与再生混凝土骨料(RCA)或电弧炉矿渣(EAFS)代替部分骨料的机械性能。使用常规的热拌沥青(HMA)和不含副产物的WMA作为参考。评估是在实验室中通过对从实际生产,铺设和压实情况下建造的实验性路面部分采集的试样进行测试而进行的。性能测试包括车轮跟踪测试,四点弯曲测试和间接拉伸强度以评估水敏感性。将有机蜡和化学表面活性剂用于降低正在研究的WMA的处理温度。除了将HMA和WMA用作参考之外,该研究还评估了将60%的RCA或30%的EAFS引入WMA共混物中以代替骨料的影响。 WMA和副产物的测试结果可以得出结论,将EAFS或RCA引入WMA混合物中会增加马歇尔稳定性,并可能增加或降低耐车辙的能力。研究结果还表明,刚度模量有所降低,耐疲劳性没有明显变化。另外,水敏感性略有降低。将这些结果与没有副产品的WMA在其他地方观察到的性能进行比较,发现添加RCA或EAFS是令人满意的。实验部分的建造使用了常规的批处理设备,摊铺机和压实机,没有任何明显的技术问题。 (C)2018 Elsevier Ltd.保留所有权利。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号