The service life of real construction elements is usually long, so the study of the behavior of cement-based materials with new pozzolanic additions in the very long term, after several hardening years, could be interesting. Here, the influence of using waste brick powder as 10% and 20% clinker substitution in microstructure and several durability-related parameters of mortars after 1500 hardening days (approximately 4 years) has been studied. According to the results obtained, the incorporation of brick powder overall improved the performance of mortars after 4 years, compared to reference mortars without addition, especially regarding the pore structure and chloride diffusion.
机译:真正的建筑元素的使用寿命通常很长,所以在几个硬化年后,长期以来,在很长远的时候研究水泥基材料的行为,经过几年,可能是有趣的。 这里,研究了使用废砖粉作为10%和20%熟料取代在组织中的10%和20%熟料替代的影响,以及在1500例硬化天(约4年)之后的迫击炮中的几个耐久性相关参数。 根据所得的结果,与参考砂浆相比,砖粉的掺入总体改善了迫击炮的性能,而没有添加,特别是关于孔隙结构和氯化物扩散。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号