This work shows how it is possible to tailor cement-rubber composites suitable as renders and masonry mortars with a reduced liquid water absorption. Recycled tyre rubber is used as aggregate in mixture with siliceous sand and its content is tuned in order to limit depletion of mechanical properties and, at the same time, ensure a sufficiently massive utilization of this secondary raw material. An extended investigation of the properties both at the fresh and hardened state is conducted. We show that presence of rubber sensitively reduces fluidity (hence workability) of the mortar. In particular, rubber modifies rheological properties such as thixotropy and dynamic torque, while does not affect viscosity. Overall, the fresh state properties are compatible with the casting and application of these mortar typologies, even for the highest rubber content (20-25% by volume). This rubber content is shown to be sufficient to ensure, just after few days of curing, an almost complete abatement of water drop absorption, specific functionality of these novel and more sustainable mortars. (C) 2020 Elsevier Ltd. All rights reserved.
机译:这项工作表明,如何以较低的液体吸水量来定制适合用作抹灰和砌筑砂浆的水泥-橡胶复合材料。再生轮胎橡胶被用作与硅砂混合的骨料,并对其含量进行了调整,以限制机械性能的降低,同时确保充分利用这种次级原料。对新鲜状态和硬化状态下的性能进行了广泛的研究。我们表明,橡胶的存在会敏感地降低砂浆的流动性(因此可加工性)。特别是,橡胶可改变流变特性,如触变性和动态扭矩,而不会影响粘度。总体而言,即使对于最高的橡胶含量(体积百分比为20%至25%),新鲜状态性能也可以与这些砂浆类型的浇铸和应用兼容。该橡胶含量显示足以在硫化几天后就足以确保几乎完全消除水滴吸收,这些新型且更具可持续性的砂浆的特定功能。 (C)2020 Elsevier Ltd.保留所有权利。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号