Failure analysis of (±55°)_3 filament wound composite pipes with an inclined surface crack under static internal pressure

机译:静态内压下(±55°)_3长丝缠绕斜管复合管的失效分析

获取原文
获取原文并翻译 | 示例
           

摘要

This study conducts failure analysis of filament wound glass reinforced plastic (GRP) pipes made of E-glass/epoxy with an inclined surface crack under open-ended internal pressure. Test specimens are composed of six antisymmetric layers with (±55°)_3 winding angles. Tests have been performed at seven different crack angles: 0°, 15°, 30", 60°, 45°, 75°, and 90°, with crack-to-thickness ratio of a/t = 0.50. The burst strengths of the specimens were determined, and the dependence of the burst strength on the crack angle was examined.
机译:这项研究进行了无端内部压力下由倾斜表面裂纹的E玻璃/环氧树脂制成的缠绕玻璃纤维增​​强塑料(GRP)管的失效分析。试样由具有(±55°)_3缠绕角的六个不对称层组成。已经在七个不同的裂纹角度下进行了测试:0°,15°,30“,60°,45°,75°和90°,裂纹与厚度的比值为a / t = 0.50。确定试样,并检查破裂强度与裂纹角度的关系。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号