Thermo- and pH-responsive semi-IPN polyampholyte hydrogels were prepared by using carboxymethyl chitosan and P(2-(dimethylamino) ethyl methacrylate) with N N'-Methylenebisacrylamide (BIS) as crosslinking agent. It was found that the semi-IPN hydrogel shrunk most at the isoelectric point (IEP) and swelled when pH deviated from the IEP. Its swelling ratio dramatically decreased between 30 and 50 °C at pH 6.8 buffer solution. It also showed good reversibility. The UV results showed that when the pH values of drug release medium were 3.7, 6.8, and 9 at 25 °C, the cumulative release rates reached 83.1, 51.5, and 72.2%, respectively. The release rate of coenzyme A (CoA) was higher at 50 °C than 37 and 25 °C at pH 6.8 solution. The release rate decreased with increasing the content of carboxymethyl chitosan at 25 °C in pH 6.8 solution. The results showed that semi-IPN hydrogel seems to be of great promise in pH/temperature drug delivery systems.
机译:通过使用羧甲基壳聚糖和P(2-(二甲基氨基)甲基丙烯酸乙酯)与N N'-亚甲基双丙烯酰胺(BIS)作为交联剂,制备了对温度和pH有响应的半IPN聚两性电解质水凝胶。已发现,半IPN水凝胶在等电点(IEP)收缩最多,并且在pH偏离IEP时膨胀。在pH 6.8缓冲溶液中,其溶胀率在30至50°C之间急剧降低。它还显示出良好的可逆性。紫外检测结果表明,当药物释放介质在25°C下的pH值为3.7、6.8和9时,累积释放率分别达到83.1%,51.5和72.2%。在pH 6.8溶液中,辅酶A(CoA)的释放速率在50°C时高于37和25°C。在25℃,pH 6.8的溶液中,释放速率随羧甲基壳聚糖含量的增加而降低。结果表明,半IPN水凝胶在pH /温度药物输送系统中似乎很有希望。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号