Synthesis and characterization of polystyrene/2-(5-chloro-2H-benzotriazole-2-yl)-6-(1,1- dimethylethyl)-4-methyl-phenol composite microspheres of narrow size distribution for UV irradiation protection

机译:窄尺寸分布用于紫外线防护的聚苯乙烯/ 2-(5-氯-2H-苯并三唑-2-基)-6-(1,1-二甲基乙基)-4-甲基苯酚复合微球的合成与表征

获取原文
获取原文并翻译 | 示例
   

获取外文期刊封面封底 >>

       

摘要

Polystyrene (PS) UV absorber microspheres of narrow size distribution have been prepared in two ways: (1) Entrapment of the UV absorber molecule, 2-(5-chloro-2H-benzotriazole-2-yl)-6-(1, 1-dimethylethyl)-4-methyl-phenol) [TINUVIN® 326] within uniform PS template microspheres by swelling these template particles with methylene chloride emulsion droplets containing the TINUVIN, followed by evaporation of the methylene chloride from the swollen PS microspheres. (2) A similar swelling process, substituting the methylene chloride emulsion droplets containing the TINUVIN for methylene chloride emulsion droplets containing the monomers, divinyl benzene (DVB) and styrene (S) and the initiator, benzoyl peroxide and TINUVIN. The monomers within the swollen microspheres were then polymerized by elevating the temperature of the swollen particles to 73 °C. The influence of the weight ratio [TINUVIN]/[PS] on the entrapped percentage of TINUVIN was elucidated. Polyethylene/TINUVIN, PE/(PS/TINUVIN), and PE/(PS/P(S-DVB-TINUVIN)) resins and films were prepared by melt blending of low-density PE with TINUVIN and with the UV absorber microspheres, followed by a tubular blown process. The UV absorption of these composite films was demonstrated. The leakage kinetics of the TINUVIN from these composite films was according to the following order: PE/(PS/P(S-DVB-TINUVIN)) < PE/(PS/TINUVIN) < PE/TINUVIN.
机译:已经通过两种方法制备了窄尺寸分布的聚苯乙烯(PS)紫外线吸收剂微球:(1)截留紫外线吸收剂分子2-(5-氯-2H-苯并三唑-2-基)-6-(1,1 -用均匀的PS模板微球中的(二甲基乙基)-4-甲基-苯酚)[TINUVIN®326],方法是将这些模板颗粒用含有TINUVIN的二氯甲烷乳液液滴溶胀,然后从溶胀的PS微球中蒸发掉二氯甲烷。 (2)类似的溶胀过程,用含有TINUVIN的二氯甲烷乳液液滴代替含有单体,二乙烯基苯(DVB)和苯乙烯(S)以及引发剂,过氧化苯甲酰和TINUVIN的二氯甲烷乳液液滴。然后通过将溶胀的颗粒的温度升高到73℃来使溶胀的微球内的单体聚合。阐明了重量比[TINUVIN] / [PS]对TINUVIN截留百分率的影响。聚乙烯/ TINUVIN,PE /(PS / TINUVIN)和PE /(PS / P(S-DVB-TINUVIN))树脂和薄膜是通过将低密度PE与TINUVIN和紫外线吸收剂微球熔融共混而制得的通过管状吹塑工艺。证明了这些复合膜的紫外线吸收。这些复合膜中TINUVIN的泄漏动力学按照以下顺序:PE /(PS / P(S-DVB-TINUVIN))