Preparation of activated carbons from cherry stones by activation with potassium hydroxide

机译:氢氧化钾活化法从樱桃石中制备活性炭。

获取原文
获取原文并翻译 | 示例
       

摘要

Using cherry stones, the preparation of activated carbon has been undertaken in the present study by chemical activation with potassium hydroxide. A series of KOH-activated products was prepared by varying the carbonisation temperature in the 400-900 degrees C range. Such products were characterised texturally by gas adsorption (N-2, -196 degrees C), mercury porosimetry, and helium and mercury density measurements. FT-IR spectroscopy was also applied. The carbons prepared as a rule are microporous and macroporous solids. The degree of development of surface area and porosity increases with increasing carbonisation temperature. For the carbon heated at 900 degrees C the specific surface area (BET) is 1624 m(2) g(-1), the micropore volume is 0.67 cm(3) g(-1), the mesopore volume is 0.28 cm(3) g(-1), and the macropore volume is 1.84 cm(3) g(-1). (c) 2005 Elsevier B.V. All rights reserved.
机译:在本研究中,已使用樱桃石通过氢氧化钾的化学活化来制备活性炭。通过在400-900摄氏度范围内改变碳化温度来制备一系列KOH活化的产品。通过气体吸附(N-2,-196摄氏度),汞孔隙率法以及氦气和汞密度测量,对此类产品进行结构表征。 FT-IR光谱法也被应用。通常制备的碳是微孔和大孔固体。表面积和孔隙率的发展程度随碳化温度的升高而增加。对于在900摄氏度下加热的碳,比表面积(BET)为1624 m(2)g(-1),微孔体积为0.67 cm(3)g(-1),中孔体积为0.28 cm(3) )g(-1),大孔体积为1.84 cm(3)g(-1)。 (c)2005 Elsevier B.V.保留所有权利。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号