Semi-circular Shaped Zno Nanowhiskers Assemblies Deposited Using An Aqueous Solution

机译:使用水溶液沉积的半圆形Zno纳米晶须组件

获取原文
获取原文并翻译 | 示例

摘要

Semi-circular shaped ZnO nanowhiskers assemblies were fabricated on a substrate by a simple bottom-up approach using an aqueous solution at 88℃. The substrate was coated with ZnO seeds derived from the thermal decomposition of zinc nitrate hexahydrate at 350℃. A 200-mL aqueous solution of 0.1 mol/L zinc nitrate hexahydrate, 0.1 mol/L hexamethylenetetramine, and 0.02 mol/L polyethylenimine was used for depositing ZnO nanowhiskers. X-ray diffraction (XRD) and a field emission scanning electron microscope (FE-SEM) were used to characterize phase and orientation, and morphology and microstructure, respectively. The pre-existing aggregated ZnO nanosheets on the substrate promoted heterogeneous nucleation and growth of ZnO nanowhiskers assemblies preferentially orientated along the c-axis direction, resulting in the formation of the semi-circular shape.
机译:通过简单的自下而上的方法,使用88℃的水溶液,在基板上制备了半圆形ZnO纳米晶须组件。在基底上涂以源自六水合硝酸锌在350℃下热分解的ZnO晶种。使用200 mL的0.1 mol / L硝酸锌六水合物,0.1 mol / L六亚甲基四胺和0.02 mol / L聚乙烯亚胺的水溶液沉积ZnO纳米晶须。 X射线衍射(XRD)和场发射扫描电子显微镜(FE-SEM)分别用于表征相和取向,形态和微观结构。在基板上预先存在的聚集的ZnO纳米片促进了ZnO纳米晶须组件的异质成核和生长,这些晶须优先沿c轴方向定向,从而形成了半圆形。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号