首页> 外文期刊>Advanced Optical Materials >Mixed Spacer Cation Stabilization of Blue-Emitting n = 2 Ruddlesden–Popper Organic–Inorganic Halide Perovskite Films
【24h】

Mixed Spacer Cation Stabilization of Blue-Emitting n = 2 Ruddlesden–Popper Organic–Inorganic Halide Perovskite Films

机译:蓝光n = 2的Ruddlesden-Pop有机-无机卤化物钙钛矿薄膜的混合间隔物阳离子稳定性

获取原文
获取原文并翻译 | 示例
获取外文期刊封面目录资料

摘要

Ruddlesden-Popper halide perovskite (RPP) materials are of significant interest for light-emitting devices since their emission wavelength can be controlled by tuning the number of layers n, resulting in improved spectral stability compared to mixed halide devices. However, RPP films typically contain phases with different n, and the low n phases tend to be unstable upon exposure to humidity, irradiation, and/or elevated temperature which hinders the achievement of pure blue emission from n = 2 films. In this work, two spacer cations are used to form an RPP film with mixed cation bilayer and high n = 2 phase purity, improved stability, and brighter light emission compared to a single spacer cation RPP. The stabilization of n = 2 phase is attributed to favorable formation energy, reduced strain, and reduced electron-phonon coupling compared to the RPP films with only one type of spacer cation. Using this approach, pure blue light-emitting diodes (LEDs) with Commission Internationale de l'eclairage (CIE) coordinates of (0.156, 0.088) and excellent spectral stability are achieved.
机译:Ruddlesden-Popper卤化物钙钛矿(RPP)材料对于发光器件非常重要,因为可以通过调整层数n来控制其发射波长,与混合卤化物器件相比,可以提高光谱稳定性。然而,RPP膜通常包含具有不同n的相,并且低n相在暴露于湿气,辐射和/或高温时趋于不稳定,这阻碍了从n = 2膜获得纯蓝色发射。在这项工作中,与单个间隔物阳离子RPP相比,使用两个间隔物阳离子形成具有混合阳离子双层且n = 2相纯度高,稳定性提高和发光更亮的RPP膜。与仅具有一种间隔阳离子的RPP膜相比,n = 2相的稳定归因于良好的形成能,降低的应变和降低的电子-声子耦合。使用这种方法,可以获得国际照明委员会(CIE)坐标为(0.156,0.088)的纯蓝色发光二极管(LED)和出色的光谱稳定性。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号