Shear Behavior and Diagonal Crack Width for Reinforced Concrete Beams with High-Strength Shear Reinforcement

机译:高强度抗剪钢筋混凝土梁的剪力特性和对角线裂缝宽度

获取原文
获取原文并翻译 | 示例
           

摘要

ACI 318-11 specifies that the yield strength of shear reinforcement be limited to 420 MPa (60,000 psi) in a shear design equation. However, this is not the case in other design codes, such as EC2-04, CSA-04, and JSCE-02, where a yield strength of shear reinforcement of more than 420 MPa (60,000 psi) is allowed in shear design. The primary reason for the limit of 420 MPa (60,000 psi) in ACI 318-11 is to provide enough transverse reinforcement and, hence, control diagonal crack width. To investigate this, a total of 18 reinforced concrete (RC) beam specimens incorporating high-strength shear reinforcement were tested and the applicability of the reinforcement was then assessed. In addition, the diagonal crack widths from the current test results and the 38 RC beam experimental results available in the technical literature have been evaluated by comparison with the crack regulation of ACI 318-11. Comparative results reveal that diagonal crack width can be influenced by the amount of shear reinforcement and compressive concrete strength. In short, the width is inversely proportional to amount of shear reinforcement divided by compressive concrete strength.
机译:ACI 318-11规定,在剪力设计方程式中,剪力增强的屈服强度应限制为420 MPa(60,000 psi)。但是,在其他设计规范(例如EC2-04,CSA-04和JSCE-02)中却不是这种情况,在剪切设计中允许超过420 MPa(60,000 psi)的剪切增强屈服强度。 ACI 318-11中限制为420 MPa(60,000 psi)的主要原因是要提供足够的横向钢筋,并因此控制对角线裂缝宽度。为了对此进行调查,总共测试了18个结合了高强度剪切钢筋的钢筋混凝土(RC)梁样本,然​​后评估了钢筋的适用性。此外,通过与ACI 318-11的裂缝规则进行比较,评估了当前测试结果和技术文献中38条RC梁实验结果得出的对角裂缝宽度。比较结果表明,斜向裂缝宽度可能受剪力和抗压混凝土强度的影响。简而言之,宽度与抗剪加固量除以抗压混凝土强度成反比。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号