Preconcentration of Fe(III) Co(II) Ni(II) Cu(II) Zn(II) and Pb(II) with ethylenediamine-modified graphene oxide

机译:Fe(III)Co(II)Ni(II)Cu(II)Zn(II)和Pb(II)用乙二胺改性的氧化石墨烯进行预浓缩

代理获取
本网站仅为用户提供外文OA文献查询和代理获取服务,本网站没有原文。下单后我们将采用程序或人工为您竭诚获取高质量的原文,但由于OA文献来源多样且变更频繁,仍可能出现获取不到、文献不完整或与标题不符等情况,如果获取不到我们将提供退款服务。请知悉。

摘要

We describe a novel solid phase sorbent that was synthesized by coupling graphene oxide (GO) to ethylenediamine (EDA). This nanomaterial (referred to as GO-EDA) is capable of adsorbing the ions of iron, cobalt, nickel, copper, zinc and lead. The ethylenediamine-modified graphene oxide was characterized by X-ray photoelectron spectroscopy, scanning electron microscopy and Fourier transform infrared spectroscopy. The analytical procedure relies on (a) sorption of metal ions on GO-EDA dispersed in aqueous samples; (b) filtering, and (c) direct submission of the filter paper to energy-dispersive X-ray fluorescence spectrometry. This kind of dispersive micro-solid phase extraction was optimized with respect to pH values, concentration of GO-EDA, contact time, and the effects of interfering ions and humic acid on recovery of determined elements. Under optimized conditions, the recoveries of spiked samples range from 90 to 98 %. The detection limits are 0.07, 0.10, 0.07, 0.08, 0.06 and 0.10 ng mL−1 for Fe(III), Co(II), Ni(II), Cu(II), Zn(II) and Pb(II), respectively. The method has a relative standard deviation of <6 %, and its accuracy was verified by analysis of two standard reference materials [LGC6016 (estuarine water) and BCR-610 (groundwater)]. It was successfully applied to the determination of trace amounts of these metal ions in water samples.>Graphical AbstractGraphene oxide was coupled to ethylenediamine in order to obtain an effective sorbent (GO-EDA) for preconcentration of Fe(III), Co(II), Ni(II), Cu(II), Zn(II) and Pb(II) from environmental water samples
机译:我们描述了一种新型的固相吸附剂,该吸附剂是通过将氧化石墨烯(GO)与乙二胺(EDA)偶联而合成的。这种纳米材料(称为GO-EDA)能够吸附铁,钴,镍,铜,锌和铅的离子。乙二胺改性的氧化石墨烯通过X射线光电子能谱,扫描电子显微镜和傅里叶变换红外光谱进行表征。分析程序依赖于(a)分散在水性样品中的GO-EDA上的金属离子吸附; (b)过滤,以及(c)将滤纸直接提交至能量色散X射线荧光光谱法。针对pH值,GO-EDA浓度,接触时间以及干扰离子和腐殖酸对所测定元素的回收率的影响,对这种分散型微固相萃取进行了优化。在优化条件下,加标样品的回收率在90%到98%之间。 Fe(III),Co(II),Ni(II),Cu(II),Zn(II)的检出限为0.07、0.10、0.07、0.08、0.06和0.10 ngmL -1 )和Pb(II)。该方法的相对标准偏差<6%,并且通过分析两种标准参考物质[LGC6016(河口水)和BCR-610(地下水)]验证了其准确性。它已成功地用于测定水中样品中的痕量金属离子。<!-fig ft0-> <!-fig @ position =“ anchor” mode = article f4-> <!-fig mode =“ anchored” f5-> >图形摘要<!-fig / graphic | fig / alternatives / graphic mode =“ anchored” m1-> <!-标题a7->氧化石墨烯与乙二胺,以便从环境水样品中获得用于预浓缩Fe(III),Co(II),Ni(II),Cu(II),Zn(II)和Pb(II)的有效吸附剂(GO-EDA)