首页> 美国卫生研究院文献>Springer Open Choice >The Influence of Viscosity and Non-freezing Water Contents Bounded to Different Hydroxypropyl Celluloses (HPC) and Hydroxypropyl Methylcelluloses (HPMC) on Stability of Acetylsalicylic Acid
【2h】

The Influence of Viscosity and Non-freezing Water Contents Bounded to Different Hydroxypropyl Celluloses (HPC) and Hydroxypropyl Methylcelluloses (HPMC) on Stability of Acetylsalicylic Acid

机译:羟丙基纤维素(HPC)和羟丙基甲基纤维素(HPMC)的黏度和非冻结水含量对乙酰水杨酸稳定性的影响

代理获取
本网站仅为用户提供外文OA文献查询和代理获取服务,本网站没有原文。下单后我们将采用程序或人工为您竭诚获取高质量的原文,但由于OA文献来源多样且变更频繁,仍可能出现获取不到、文献不完整或与标题不符等情况,如果获取不到我们将提供退款服务。请知悉。

摘要

The aim of the study was to examine the influence of non-freezing water (NFW) contents bound to hydroxypropyl methylcellulose (HPMC) or hydroxypropyl cellulose (HPC) binary mixtures using acetylsalicylic acid (ASA) as a model moisture-sensitive ingredient. Polysaccharides with significantly different physicochemical properties were mixed with acetylsalicylic acid at a ratio 1:1 (w/w). The measurements of NFW contents of hydrated samples were carried out using differential scanning calorimetry (DSC). In the method used, the dry mass normalized dependency of melting enthalpy (ΔH) and respective contents of water was found to be linear. NFW values were calculated after extrapolation ΔH to 0. For stability studies, HPC/ASA and HPMC/ASA mixtures were stored at 40°C and 75% RH for 5 weeks in the climatic chamber. The ASA hydrolysis was investigated using UV-Vis spectrophotometry. The amounts of NFW calculated for raw HPMC 3 cP and 100,000 cP were 0.49 and 0.42 g g−1, while for polymer and ASA mixtures, prepared from HPC type LF (126 cP) and MF (6300 cP) as well as from HPMC 3 cP and 100,000 cP were 0.23, 0.28 g g−1, 0.21 g g−1, and 0.33 g g−1 respectively. The measured NFW values were connected with appropriate concentrations of unhydrolyzed ASA.
机译:该研究的目的是使用乙酰水杨酸(ASA)作为模型水敏成分,研究与羟丙基甲基纤维素(HPMC)或羟丙基纤维素(HPC)二元混合物结合的非冷冻水(NFW)含量的影响。将具有明显不同的理化性质的多糖与乙酰水杨酸以1:1(w / w)的比例混合。使用差示扫描量热法(DSC)对水合样品的NFW含量进行测量。在所使用的方法中,发现熔融焓(ΔH)和水各自含量的干质量归一化依赖性是线性的。在将ΔH外推至0后计算NFW值。为进行稳定性研究,将HPC / ASA和HPMC / ASA混合物在40°C和75%RH的条件下在气候室内存放5周。使用UV-Vis分光光度法研究了ASA的水解。计算得出的原始HPMC 3 cP和100,000 cP的NFW量分别为0.49和0.42 g g -1 ,而对于聚合物和ASA混合物,则由LF(126 cp)和MF(6300 cp)HPC类型制备)以及HPMC 3 cP和100,000 cP分别为0.23、0.28 g g -1 ,0.21 g g -1 和0.33 g g -1 。测得的NFW值与适当浓度的未水解ASA相关。