Water washing of cottonseed meal is more cost-efficient and environmentally friendly than protein isolation by means of alkaline extraction and acidic precipitation. Thus, water-washed cottonseed meal (WCSM) is more promising as biobased wood adhesives. In this work, we examined the effects of the particle size on the morphology and adhesive performance of WCSM. Pilot-scale produced and dried WCSM was treated by three grinding methods: (1) ground by a hammer mill and passed through a 0.5-mm screen, (2) further ground by a cyclone mill and passed through a 0.5-mm screen, or (3) further ground by a ball mill and passed through a 0.18-mm screen. Micro-morphological examination revealed two types of particles. The filament-like particles were mainly fibrous materials from residual linters. Chunk-like particles were more like aggregates or accumulations of small particles, with proteins as the major component. Further grinding of the 0.5-mm Hammer product with the Cyclone and Ball mill led to more fine (smaller) particles in the WCSM products. The impact of further grinding on the dry and soaked adhesive strengths was minimal. However, the decrease of the hot and wet strengths of WCSM products by the additional grinding was significant (p ≤ 0.05). Data presented in this work is useful in developing the industrial standards of WCSM products used in wood bonding.
机译:与通过碱性提取和酸性沉淀进行蛋白质分离相比,棉籽粕的水洗具有更高的成本效益和环境友好性。因此,水洗棉籽粉(WCSM)作为生物基木材胶粘剂更有希望。在这项工作中,我们检查了粒径对WCSM的形态和粘合性能的影响。用三种研磨方法处理中试生产和干燥的WCSM:(1)用锤磨机研磨并通过0.5毫米的筛子;(2)用旋风磨机进一步研磨并通过0.5毫米的筛子;或(3)用球磨机进一步研磨并通过0.18毫米的筛网。微观形态检查显示出两种类型的颗粒。长丝状颗粒主要是来自残留棉绒的纤维材料。块状颗粒更像是小颗粒的聚集或堆积,其中蛋白质为主要成分。使用Cyclone and Ball研磨机进一步研磨0.5毫米锤产品会导致WCSM产品中出现更多细小颗粒。进一步研磨对干燥和浸泡的粘合强度的影响很小。但是,通过额外研磨,WCSM产品的湿强度和湿强度会显着降低(p≤0.05)。这项工作中提供的数据对于制定用于木材粘合的WCSM产品的工业标准很有用。