Background: The purpose of this study was to identify the basic physical properties of 3 commonly available tissue-conditioning materials to gain knowledge for their clinical use as impression materials.Materials & Methods: A total of 60 samples were prepared and each sample was mixed and prepared according to manufacture direction. Finally five specimens of each tissue conditioners were subjected for each of the above test at different time duration.Results & Conclusion: The study showed that all the materials underwent water loss from the time of mixing to 24 hr & became hard. The plasticity of coecomfort & viscogel decreased from the time of mixing upto 1hr & 2hr respectively & again increased after that till 24 hrs, but the softone showed decreased plasticity after 30 min till 24hrs.Softone & coecomfort at 30 min showed better flow & more plasticity than that of viscogel. The dimensional accuracy of softone & viscogel at 30min is better than that of coecomfort.Thus softone at 30 min after mixing has better Dimensional accuracy, Plasticity and Flow; suitable for making functional impression then that of Coe-comfort and Viscogel.How to cite this article: Shylesh K B S, Hallikerimath R B, Rajeev V V, Ganesh S, Meenakshi S. Evaluation of Physical Properties of Tissue Conditioning Materials as used in Functional Impression - A Lab Study. J Int Oral Health 2013; 5(3):20-27.
机译:背景:本研究的目的是确定3种常用的组织调理材料的基本物理特性,以了解其作为印模材料的临床应用知识。材料与方法:总共准备了60个样品,并将每个样品混合并根据制造说明进行制备。最后,每个组织调节剂的五个标本分别在不同的时间进行上述测试。结果与结论:研究表明,从混合到搅拌24小时,所有材料都发生了失水。变得很难。混合至1小时和2小时时,舒适感和粘胶的可塑性分别下降,直到24小时后再次增加,但软胶在30分钟至24小时后显示出可塑性下降.30分钟的软质和舒适感显示出更好的流动性和更大的可塑性比黏胶。柔软剂和粘胶在30分钟时的尺寸精度要比同感舒适性好。因此,混合后30分钟时的柔软剂具有更好的尺寸精度,可塑性和流动性; 如何引用本文: Shylesh KBS,Hallikerimath RB,Rajeev VV,Ganesh S,MeenakshiS。组织调理材料的物理性能评估用于功能印象-实验室研究。 《国际口腔卫生杂志》 2013; 5(3):20-27。