This paper presents an innovative application for spent coffee grounds (SCGs) used as filler for the formulation of lightweight clay ceramic aggregates (LWA). LWA can be used for urban and agricultural purposes as a sustainable solution. Spent coffee grounds were tested as a pore forming agent partially acting as a replacement for red clay in material formulation before firing. Substitutions of 10, 15, and 20 wt.% of red clay were tested. The properties of lightweight aggregates with 15 wt.% of SCGs were improved using a specifically tailored fertilizer glass due to its low pH and conductivity within the soil tolerance range. Packaging glassy sand, cattle-bone flour ash, and potassium carbonate were mixed and melted in order to obtain this glass, which when added to the clayey batch functionalized the aggregates by phosphorus and potassium nutrients. The results (in particular, porosity and bulk density) show that the lightweight aggregates obtained have interesting properties for possible uses both in urban (e.g., green roofs as a drainage layer) and agricultural purposes. Moreover, pH and conductivity are in line with the Italian Standard regarding soil amendment (D.lgs. 75/2010). In addition, several leaching tests were performed in a solution containing 2 vol.% citric acid (C H O ) to evaluate the release capacity not only of nutrients (P and K) but also to check the presence and release of heavy metals, such as lead (Pb), that may come from the glassy precursor. The results obtained showed that nutrients are efficiently released in 21 days (P = 87.73% and K = 25.74% of released percentage) and Pb release is under the standard threshold of 30 ppm.
机译:本文提出了一种用于废咖啡渣(SCG)的创新应用,该咖啡渣用作配制轻质粘土陶瓷骨料(LWA)的填料。 LWA可作为可持续解决方案用于城市和农业目的。测试了用过的咖啡渣作为成孔剂,在焙烧前部分替代了材料配方中的红粘土。测试了10、15和20重量%的红粘土的替代。使用特制的肥料玻璃可改善具有15%(重量)SCG的轻质骨料的性能,因为它的pH值低且在土壤耐受范围内具有导电性。将包装的玻璃砂,牛骨粉灰和碳酸钾混合并融化,以获得这种玻璃,将其添加到黏土中时,可通过磷和钾养分对聚集体进行功能化。结果(特别是孔隙率和堆积密度)表明,所获得的轻质集料具有令人感兴趣的性质,可用于城市(例如,用作排水层的绿色屋顶)和农业用途。此外,pH和电导率符合关于土壤改良剂的意大利标准(D.lgs。75/2010)。此外,在含有2%(体积)柠檬酸(CHO)的溶液中进行了多次浸出试验,不仅评估了养分(P和K)的释放能力,还检查了重金属(例如铅)的存在和释放。 (Pb),可能来自玻璃状前体。获得的结果表明,营养素在21天之内有效释放(P = 87.73%,K =释放百分比的25.74%),Pb的释放低于30 ppm的标准阈值。