首页> 美国卫生研究院文献>Materials >Properties of Concrete Prepared with Recycled Aggregates Treated by Bio-Deposition Adding Oxygen Release Compound
【2h】

Properties of Concrete Prepared with Recycled Aggregates Treated by Bio-Deposition Adding Oxygen Release Compound

机译:生物沉积加氧释放化合物处理再生骨料制备混凝土的性能

代理获取
本网站仅为用户提供外文OA文献查询和代理获取服务,本网站没有原文。下单后我们将采用程序或人工为您竭诚获取高质量的原文,但由于OA文献来源多样且变更频繁,仍可能出现获取不到、文献不完整或与标题不符等情况,如果获取不到我们将提供退款服务。请知悉。

摘要

Recycled aggregates have high water absorption and crushing index. In order to improve the properties of recycled aggregates in concrete production, various treatments were used to modify the aggregates. In recent years, bio-deposition as a new treatment method of recycled aggregates was environmentally friendly. An improved method of bio-deposition was implemented to modify the properties of recycled mortar aggregates (RMA). O-bio-deposition is based on aerobic bacteria induced CaCO3 precipitation by respiration by varying the distance between the RMA and the bottom of the container and by adding an oxygen release compound to the culture solution that contains bacteria to promote the induction of CaCO3. First, the physical properties, including water absorption, crushing value, and apparent density, of the coarse RMA under different treatment methods were determined, and an o-bio-deposition treatment method was obtained. The fine RMA was treated and compared with the untreated RMA. Concretes were then prepared from the treated coarse RMA, and compressive strength and slump were determined. In addition, the effect of the o-bio-deposition treatment on the RMA surface and the micro-cracks of concretes were observed by scanning electron microscopy (SEM). It was found that the water absorption and crushing index of the coarse RMA treated by o-bio-deposition were reduced by 40.38 and 19.76% compared with untreated RMA, respectively. Regarding the concrete, the slump and the compressive strength (28 d) of concrete were increased by 115% and 25.3%, respectively compared with the untreated concrete.
机译:再生骨料具有高吸水率和破碎指数。为了改善混凝土生产中再生骨料的性能,采用了各种处理方法来改性骨料。近年来,生物沉积作为一种再生骨料的新处理方法对环境友好。实施了一种改进的生物沉积方法,以改善再生砂浆骨料(RMA)的性能。 O-生物沉积基于需氧细菌,通过改变RMA与容器底部之间的距离并通过向包含细菌的培养液中添加氧气释放化合物以促进CaCO3的诱导作用来进行呼吸作用来诱导CaCO3沉淀。首先,确定了在不同处理方法下粗糙RMA的物理性能,包括吸水率,压碎值和表观密度,并获得了o-生物沉积处理方法。将细RMA处理并与未处理RMA进行比较。然后从处理过的粗糙RMA制备混凝土,并确定抗压强度和坍落度。另外,通过扫描电子显微镜(SEM)观察了o-生物沉积处理对RMA表面和混凝土微裂纹的影响。结果表明,与未经处理的RMA相比,经邻位生物沉积处理的粗RMA的吸水率和压碎指数分别降低了40.38和19.76%。关于混凝土,与未处理的混凝土相比,混凝土的坍落度和抗压强度(28 d)分别增加了115%和25.3%。