通过对硼硅酸系玻璃与钛酸铝陶瓷复合,制备了性能较优的复合材料,在较低的烧成温度750℃下,介电常数为4.19,热膨胀系数为(3.23±0.02)×10<'-6>/℃.%Composite material compounded by borosilicate glass and aluminum titanate ceramic is obtained with better performance at a relatively low sintering temperature of 750 ℃. The dielectric constant is 4. 19, thermal expansion coefficient is (3.23±0.02)× 10-6.