Coercive Force and Antimagnetizing Mechanism Relating to Size of Ferromagnetic Microcrystal--A Consummating to Result of Stoner-Wohlforth Theory

         

摘要

The expression of critical size of ferromagnetic microcrystal in an external magnetic field with an intensity of H is derived by means of comparing energies of domain structure states.The ferromagnetic microcrystal here means an ferromagnetic single crystal with the size which is smaller than L0, and L0 is the critical value of the size of single-domain particles at the external magnetic field intensity H =0.Also, the coercive strength H(Ls) relating to the size of microcrystal Ls is given and quantitatively evaluated with the material SmCo5 as an instance.It is thus concluded that if L0 > Ls > LC, the antimagnetization of microcrystal will be subjected to a multi-domain process just like the particles of a size greater than L0, only if Ls < LC, the anti-magnetizaton will be carried on in accordance with the Stoner-Wohlforth mechanism( LC is the maximum size of microcrystal with MHcth ).It is suggested that the material RECo5 is available to make an advanced magnet with MHC = 2 K/Mc.

著录项

获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号