In terms of consolidant protection of earthern architectural sites in humid environment,it is still at the stage of exploration in our country.Combaining with characteristics of consolidant project of earthern sites,this paper on the basis of consolidant techniques from JiaoHe Ancient City campaign makes an ascertainment to PS permeability property and consolidant effects at different moisture content by means of testing infiltration of the soil of JiaoHe Ancient City site for different moisture content.Prior to prepare remoulding samples of 1.40 to 1.45 g/cm3 for density,19%,17%,15%,13%,11%,9%,7%,5%,3%,1% for moisture content with site soil,then utilize PS solution at the modulus of 3.85 and the concentration of 5% to infiltrate into each sample respectively,and meanwhile test infiltration deformation,infiltration capacity and infiltration speed,then test resilience wave and unconfined pressive strength until samples to be completely dry in the air and analysis permeability property and consolidant effect of PS solution to site soil at different moisture content.The results of test manifest that it differs a lot for infiltration deformation,infiltration capacity,infiltration speed and intensity heightening of PS solution aider infiltration at different moisture content and illustrates certain regularities.The initial conclusion is that PS can adapt to consolidate architectural sites at the moisture contenof 3%~9%.
机译:从土工地加固工程的特点来看,结合Jia河古城运动的加固技术,结合土工地加固工程的特点,提出了在湿润环境下对土工建筑物的加固保护还处于探索阶段。通过测试Jia河古城遗址不同水分含量的土壤入渗性,确定不同水分含量下PS的渗透性和固结效果。在制备密度为1.40至1.45 g / cm3的重塑样品之前,密度分别为19%,17%场地土壤的含水量分别为15%,13%,11%,9%,7%,5%,3%,1%,然后利用模量为3.85,浓度为5%的PS溶液渗透到每个土壤中分别测试样品,同时测试入渗变形,入渗能力和入渗速度,然后测试回弹波和无侧限抗压强度,直到样品在空气中完全干燥并分析渗透性a试验结果表明,PS溶液对不同水分含量的PS溶液的入渗变形,入渗能力,入渗速度和强度升高有很大的不同,并说明了一定的规律性。初步结论是,聚苯乙烯在3%〜9%的水分含量下能够适应建筑工地的固结。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号