Fabrication of BSA loaded Poly(Caprolactone) (PCL) Microsphere Incorporated Chitosan Scaffolds for Tissues Engineering Application

机译:BSA加载聚(己内酮)(PCL)微球的制备催化壳聚糖支架用于组织工程应用

获取原文

摘要

Scaffolds-based tissues engineering involves the combination of an artificial extracellular matrix (ECM), living cells, with high porosity and well connected pores that will provide suitable environment for cells. In this study, firstly, poly(caprolactone) (PCL)-based microspheres were synthesized and characterized. Bovine serum albumin (BSA) (0.04% w/v) was added into the microspheres produced from 5% (w/v) PCL concentration. BSA loaded microspheres were then incorporated into chitosan solution to fabricate porous scaffolds. The scaffolds were then characterized using different techniques.
机译:基于支架的组织工程涉及人造细胞外基质(ECM),活细胞,具有高孔隙率和孔连接的孔的组合,其将为细胞提供合适的环境。在该研究中,首先,合成并表征基于聚(己内酯)(PCL)的微球。将牛血清白蛋白(BSA)(BSA)(0.04%w / v)加入到5%(w / v)pcl浓度产生的微球中。然后将BSA负载的微球掺入壳聚糖溶液中以制造多孔支架。然后使用不同的技术表征支架。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号