In this paper, experimental results are presented from an investigation of the parameters of a ceramic-faced armour system that are required to induce damage in a tungsten carbide penetrator. Experiments consisted of firing the 14.5 mm BS41 tungsten carbide cored projectile into various thicknesses and types of alumina and silicon carbide, backed by aluminium alloy semi-infinite witness plate. In each case, the ballistic resistance of the ceramic-faced armour configuration was assessed by the calculation of a differential efficiency factor. The failure of the projectile, depth of penetration and fracture morphology of the ceramic tile are also presented. Conclusions are drawn on the nature of round defeat.
机译:在本文中,提出了实验结果,从调查陶瓷面盔甲系统的参数提出,这些铠装的铠装系统需要诱导碳化钨渗透器损伤。实验包括将14.5mm BS41碳化钨芯片射击成各种厚度和类型的氧化铝和碳化硅,由铝合金半无限见证板背板。在每种情况下,通过计算差分效率因子来评估陶瓷脸部构造的抗突抗性。还介绍了陶瓷瓷砖的射弹,渗透深度和骨折形态的失效。结论是关于圆形失败的本质。

著录项

相似文献

  • 外文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号