EXPERIMENTAL STUDY OF LASER-INDUCED PROTRUSION IN HEAT-ASSISTED MAGNETIC RECORDING

机译:激光诱导突起在热辅助磁记录中的实验研究

获取原文

摘要

In heat-assisted magnetic recording (HAMR), a laser is introduced to create a hot spot on the media and locally heat the magnetic layer to its Curie temperature. Besides the optical power that the laser provides to the media, thermal energy diffuses inside the slider and induces an extra protrusion, which is called laser-induced protrusion (LIP). The LIP needs to be considered and compensated during flying in the HAMR conditions. In this study, we focus on long timescale (milliseconds) of laser heating during the flying condition. When the laser is switched from OFF to ON, the touchdown power, indicated by an acoustic emission (AE) sensor, decreases due to spacing loss and the touchdown power change (ATDP) is used as the measure of the LIP. A component-level spinstand stage for HAMR heads and media is used to study the LIP as a function of laser-on time, laser current and linear velocity. Our experimental results show that it takes around 20 ms for the LIP to reach steady state and the protrusion size is proportional to the square of laser current. As the operating linear velocity increases from 12 m/s to 24 m/s, the LIP decreases by approximately 52%.
机译:在热辅助磁记录(HAMR)中,引入激光器以在介质上产生热点,并将磁性层局部加热到其居里温度。除了激光器向介质提供的光功率之外,在滑块内部的热能扩散并引起额外的突起,称为激光诱导的突起(唇)。在HAMR条件下飞行期间,需要考虑和补偿唇部。在这项研究中,我们专注于在飞行条件下的长时间的激光加热时间(毫秒)。当激光从OFF切换到ON时,由声发射(AE)传感器指示的触控功率,由于间距损耗和触地功率变化(ATDP)减小,用作唇缘的量度。用于HAMR头部和介质的组件级旋转台阶段用于研究唇唇作为激光接通时间,激光电流和线性速度的函数。我们的实验结果表明,唇部达到稳定状态约为20毫秒,突出尺寸与激光电流的平方成比例。随着操作的线性速度从12m / s增加至24 m / s,唇缘降低约52%。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号