Two kinds of Cemented carbide tools were used to turn Iron-based superalloy GH2132 at 80 m/min-210 m/min under dry cutting condition. Infrared thermometer was used to measure cutting temperature, Tool wear was observed by SEM, and oxygen element distribution of tool surface was analyzed by EDS. Adhesive wear oxidation wear were the main wear mechanisms of the coated cemented carbide tool, Adhesive wear, abrasive were the main wear mechanisms of the carbide tool. Oxidation wear occurs above a certain temperature about 430°C, the higher the temperature the more serious the oxidation wear is. The results might be helpful to guiding the design and selection of tool materials and control of tool wear in high speed machining processes.
机译:在干切削条件下,使用两种硬质合金工具在80 m / min-210米/分钟下将基于铁基超合金GH2132变动。红外温度计用于测量切削温度,通过SEM观察刀具磨损,并通过EDS分析工具表面的氧元素分布。粘合剂耐磨氧化磨损是涂层硬质合金工具的主磨损机构,粘合剂磨损,磨料是碳化物工具的主磨损机制。氧化磨损发生在约430℃的一定温度上方,温度越高,氧化磨损越严重。结果可能有助于引导工具材料的设计和选择和高速加工过程中的工具磨损控制。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号