The structural characteristics of zeolite 4A make it to be the potential warm mix asphalt additive. Zeolite 4A containing crystal water can be synthesized with fly ash (FA) by fusion with sodium hydroxide prior to hydrothermal reaction. The influence of some factors on the water loss of synthesized zeolite 4A was investigated. The results indicate that the best technological conditions of synthesizing zeolite 4A containing crystal water with fly ash are as follows: the molar ratio of SiO_2/Al_2O_3 is 1.9; the molar ratio of Na_2O/SiO_2 is 2.0; the molar ratio of H20/Na20 is 50; under the aging temperature of 65°C, the optimum aging time is 3 h; under the crystallization temperature of 90°C, the optimum crystallization time is 4 h.
机译:沸石4A的结构特征使其成为潜在的温拌沥青添加剂。包含结晶水的沸石4A可以在水热反应之前通过与氢氧化钠熔融而与粉煤灰(FA)合成。研究了一些因素对合成沸石4A失水量的影响。结果表明,粉煤灰合成含结晶水的沸石4A的最佳工艺条件为:SiO_2 / Al_2O_3的摩尔比为1.9; SiO_2 / Al_2O_3的摩尔比为1.9。 Na 2 O / SiO 2的摩尔比为2.0。 H 2 O / Na 2 O的摩尔比为50。在65℃的时效温度下,最佳时效时间为3 h。在90℃的结晶温度下,最佳结晶时间为4小时。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号