Effect of Bombyx mori's Sericin Immobilization over Poly (L-Lactic Acid) Surface on Mesenchymal Stem Cells Attachment and Proliferation

机译:家蚕丝胶蛋白固定在聚(L-乳酸)表面对间充质干细胞附着和增殖的影响

获取原文

摘要

Poly(L-lactic acid) or PLLA as one of tissue engineering material have demonstrated low cell interaction capability due to its hydrophobicity. Bombyx mori's sericin, a polymer protein that has strongly polar side groups such as hydroxyl, carboxyl and amino groups, have been known to accelerate cells attachment and proliferation. The aim of this study was to investigate the effect of Bombyx mori's sericin immobilization with different concentration over PLLA surface on attachment and proliferation of mesenchymal stem cells (MSCs). Three concentration of sericin (2.5, 5, and 10 mg/ml) were applied on PLLA surface modification using carbodiimide chemistry. Surface characterization using Fourier Transform-Infrared Spectroscopy (FTIR) and water contact angle was performed to observe the changes on surface-modified PLLA. The MSCs attachment after 4 hours in culture and proliferation rate in 2 days were determined using hemocytometer. FTIR graphs showed that sericin was succesfully immobilized on PLLA surface. Contact angle measurement showed significant increases of the hydrophilicity on sericin-modified PLLA surfaces. MSCs attached to sericin-modified PLLA was higher in number than the cell attached on control PLLA (p0.05). However, the proliferation rate of sericin-modified PLLA has no significant differences with control PLLA (p>0.05). The conclusion was Bombyx mori's sericin application over PLLA surface enhanced MSCs attachment, but did not enhanced their proliferation rate.
机译:作为组织工程材料之一的聚(L-乳酸)或PLLA由于其疏水性而显示出低的细胞相互作用能力。家蚕丝胶蛋白是一种具有强极性侧基(例如羟基,羧基和氨基)的高分子蛋白,已知可加速细胞附着和增殖。这项研究的目的是研究不同浓度的桑蚕丝胶蛋白固定在PLLA表面上对间充质干细胞(MSCs)附着和增殖的影响。使用碳二亚胺化学法将三种浓度的丝胶(2.5、5和10 mg / ml)应用于PLLA表面改性。使用傅里叶变换红外光谱(FTIR)和水接触角进行表面表征,以观察表面改性的PLLA的变化。使用血细胞计数器测定培养4小时后的MSC附着和2天内的增殖速率。 FTIR图显示丝胶已成功固定在PLLA表面。接触角测量结果表明,丝胶修饰的PLLA表面的亲水性显着提高。附着于丝胶蛋白修饰的PLLA上的MSC数量高于附着于对照PLLA上的细胞(p0.05)。但是,丝胶蛋白修饰的PLLA的增殖速率与对照PLLA相比无显着差异(p> 0.05)。结论是家蚕的丝胶蛋白在PLLA表面上的应用增强了MSC的附着,但并未提高其增殖速率。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号