A method based on fluidizing for modifying and preparing low-cost titanium powders for 3D printing includes: using hydrogenated-dehydrogenated irregularly-shaped titanium powders as the raw material, adding the titanium powders to a fluidized bed reactor, and introducing Ar or H2 at the flow rate of 0.5-1.5 L/min, heating the reactor to 300-700° C., and fluidizing for 5-90 min to modify the titanium powders. When filled with high-purity argon gas and heated at high temperature, the sharp edges and corners of irregularly-shaped titanium powders are ground collision of the particles due to the friction among powder particles.
机译:一种用于改性和制备用于3D印刷的低成本钛粉末的流化的方法包括:使用氢化脱氢不规则形状钛粉末作为原料,将钛粉末加入流化床反应器,并引入AR或H 2 以0.5-1.5L / min的流速,加热反应器至300-700℃,并流化5-90 min以改变钛粉末。 当填充高纯度氩气并在高温下加热时,由于粉末颗粒之间的摩擦,不规则形状的钛粉末的尖锐边缘和拐角是颗粒的研磨。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号