首页> 外国专利> LIGHTENED CEMENTING SOLUTION, CEMENTING SOLUTION FOR PRODUCTIVE ZONE OF WELL AND METHOD FOR CEMENTING WELLS

LIGHTENED CEMENTING SOLUTION, CEMENTING SOLUTION FOR PRODUCTIVE ZONE OF WELL AND METHOD FOR CEMENTING WELLS

机译:轻质固井解决方案,井的生产区固井解决方案及固井方法

摘要

FIELD: oil and gas industry.;SUBSTANCE: lightened cementing solution has Portland cement, lightening admixture, aluminum oxychloride and water, as lightening admixture has admixture from the group: clay, Tripoli powder, diatomite, vermiculite, perlite, and as aluminum oxychloride has at least one compound from the group: aluminum hydrooxychloride, aluminum pentaoxychloride, aluminum tetraoxychloride with following ratio of components in portions of mass: Portland cement - 100, said lightening admixture - 5-10, said aluminum oxychloride - 0.05-1, water - until receiving water-cement relation - 0.6-1.4. Cementing solution for productive well zone has Portland cement, aluminum oxychloride and water, as aluminum oxychloride has at least one compound from the group: aluminum hydrooxychloride, aluminum pentaoxychloride, aluminum tetraoxychloride, and, additionally, water-loss decreasing substance and antifoaming additive, with following ratio of components in portions of mass: Portland cement - 100, said aluminum oxychloride - 0.05-4, water loss decreasing substance - 0.2-0.6, antifoaming additive - 0.02-0.06, water - until receiving water-cement relation 0.45-0.50, while said cementing solution can additionally contain accelerator and/or plasticizer in amounts 0.04-0.6 portions of mass each. Method for cementing wells includes washing with buffer solution with following feeding of cementing solution, after washing by buffer solution serial feeding of condensed pack of cementing solution is performed - metal silicate, said lightened cementing solution, and then said cementing solution for productive well zone. Cementing solution for productive well zone can additionally contain accelerator and/or plasticizer in amounts 0.04-0.6 portions of mass of each.;EFFECT: full filling and reliable engagement of stone with rock and casing string.;3 cl, 11ex, 2 tbl
机译:领域:石油和天然气工业;物质:减亮的胶结剂溶液包括波特兰水泥,减亮剂,氯氧化铝和水,因为减亮剂具有以下组中的混合物:粘土,的黎波里粉末,硅藻土,ver石,珍珠岩以及氯氧化铝选自以下组中的至少一种化合物:氢氯化铝,五氧氯化铝,四氧氯化铝,其在质量分数中的组分比例如下:硅酸盐水泥-100,所述减光剂-5-10,所述氯氧化铝-0.05-1,水-直至接收水灰关系-0.6-1.4。用于生产井区的固井溶液含有波特兰水泥,三氯氧化铝和水,这是因为三氯氧化铝具有以下至少一种化合物:氢氯氧化铝,五氧化氯铝,四氧化氯铝,此外,还包括减水减水物质和消泡添加剂,以及以下成分在质量中的比例:波特兰水泥-100,所说的氯氧化铝-0.05-4,减水减量物质-0.2-0.6,消泡添加剂-0.02-0.06,水-直到获得水灰关系0.45-0.50,而所述固井溶液可以另外包含各自含量为0.04-0.6质量份的促进剂和/或增塑剂。固井的方法包括以下步骤:在注入固井溶液之后,用缓冲溶液洗涤,在通过缓冲溶液洗涤之后,连续注入固结溶液的浓缩包-金属硅酸盐,所述轻质固井溶液,然后用于生产井区的所述固井溶液。用于生产井区的固井溶液可以另外包含促进剂和/或增塑剂,其含量为每种质量的0.04-0.6部分;效果:石头与岩石和套管柱的完全填充和可靠接合; 3 cl,11ex,2 tbl

著录项

  • 公开/公告号RU2255204C1

    专利类型

  • 公开/公告日2005-06-27

    原文格式PDF

  • 申请/专利权人

    申请/专利号RU20040104569

  • 发明设计人 KOSHELEV V.N.;RJABOVA L.I.;NIZHNIK A.E.;

    申请日2004-02-16

  • 分类号E21B33/138;

  • 国家 RU

  • 入库时间 2022-08-21 22:02:03