摘要

PROBLEM TO BE SOLVED: To firmly join inorganic stocks such as metal by a simple method even if firing is performed at low temperature and under low pressure.;SOLUTION: Disclosed is the joining agent for inorganic stocks composed of paste comprising metal colloid particles and a solvent, wherein the metal colloid particles are composed of metal nanoparticles (A) and a dispersant (B), further, the metal nanoparticles (A) have the number average particle diameter of ≤50 nm and also have the particle diameter of 100 to 200 nm. The metal nanoparticles (A) are composed of the metal nanoparticles (A1) with the particle diameter less than 100 nm and the metal nanoparticles (A2) with the particle diameter of 100 to 200 nm. Also, the volume ratio of both may satisfy the former/the latter=90/10 to 30/70. The joined body of inorganic stocks obtained by sintering the joining agent for inorganic stocks while interposed between the inorganic stock (C1) and the inorganic stock (C2) is firmly joined.;COPYRIGHT: (C)2011,JPO&INPIT
机译:解决的问题:即使在低温和低压下进行煅烧,也可以通过简单的方法牢固地接合金属等无机材料。解决方案:公开了一种用于无机材料的接合剂,该接合剂由包含金属胶体颗粒和金属的胶浆组成。其中金属胶体颗粒由金属纳米颗粒(A)和分散剂(B)组成的溶剂,此外,金属纳米颗粒(A)的数均粒径为50 nm,并且粒径为100至200纳米金属纳米颗粒(A)由粒径小于100nm的金属纳米颗粒(A1)和粒径为100至200nm的金属纳米颗粒(A2)组成。而且,两者的体积比可以满足前者/后者= 90/10至30/70。通过烧结无机原料接合剂并同时介于无机原料(C1)和无机原料(C2)之间而获得的无机原料接合体牢固地接合。;版权所有:(C)2011,JPO&INPIT

著录项

  • 公开/公告号JP2011094223A

    专利类型

  • 公开/公告日2011-05-12

    原文格式PDF

  • 申请/专利权人 MITSUBOSHI BELTING LTD;

    申请/专利号JP20090267997

  • 发明设计人 ISEDA TAISUKE;IZUMOTO MASAHIRO;

    申请日2009-11-25

  • 分类号B22F7/08;B22F1/02;H01B1/22;B22F9/24;

  • 国家 JP

  • 入库时间 2022-08-21 18:25:02

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号