Evaluation method null expression of haidorotarusaito based hydration metal chemical compound and the production manner, and the addition reaction catalytic converter, and this catalytic converter of the alkylene oxide which calcines this

机译:煅烧后的环氧烷烃的卤代金枪鱼基水合金属化合物的评价方法无效表达及其制造方法,加成反应催化转化器和该催化转化器

摘要

PROBLEM TO BE SOLVED: To obtain a catalyst which is excellent in a reaction rate and reaction selectivity in the additional reaction of alkylene oxide.;SOLUTION: Magnesium hydroxide or basic or neutral magnesium carbonate as a magnesium source and aluminum hydroxide as an aluminum source are brought into hydrothermal reaction at 120 to 300°C to obtain a hydrotalcite based hydrated metallic compound. The obtained hydrotalcite based hydrated metallic compound is fired at 400 to 800°C into a catalyst for the additional reaction of alkylene oxide to an active hydrogen atom-containing compound. Further, a storing base titration agent of 0.1 to 10 mol/L is dropped to a suspension obtained by adding a hydrotalcite based hydrated metallic compound to an acid aqueous solution prepared to a standard concentration of 0.001 to 0.1 mol/L so that the concentration of 0.05 to 2 wt.% can be obtained, and the pH of the suspension is measured by potentiometric titration with a glass electrode. In this case, the performance of the catalyst is evaluated from the consumption of hydroxide ions required to an inflection point of pH=10.3 from pH=7.;COPYRIGHT: (C)2004,JPO
机译:解决的问题:为了获得在环氧烷的另外的反应中反应速率和反应选择性优异的催化剂。解决方案:氢氧化镁或碱性或中性碳酸镁作为镁源,氢氧化铝作为铝源。将其在120至300℃下进行水热反应以获得水滑石基水合金属化合物。将获得的基于水滑石的水合金属化合物在400至800℃下烧成催化剂,以使环氧烷与含活性氢原子的化合物另外反应。此外,将0.1-10mol / L的储存碱滴定剂滴加到通过将水滑石基水合金属化合物添加到制备的标准浓度为0.001-0.1mol / L的酸水溶液中而获得的悬浮液中,使得可以得到0.05至2重量%,并且通过用玻璃电极的电位滴定法测量悬浮液的pH。在这种情况下,根据从pH = 7到拐点pH = 10.3所需的氢氧根离子的消耗来评估催化剂的性能。版权所有:(C)2004,JPO

著录项

  • 公开/公告号JP4585163B2

    专利类型

  • 公开/公告日2010-11-24

    原文格式PDF

  • 申请/专利权人 神島化学工業株式会社;

    申请/专利号JP20020135531

  • 发明设计人 田里 伊佐雄;松井 誠二;

    申请日2002-05-10

  • 分类号C01F7/00;B01J21/10;C07C41/03;C07C43/11;

  • 国家 JP

  • 入库时间 2022-08-21 18:18:10