PURPOSE: A high efficient sulfuric acid leaching method of uranium ore by addition ferric sulfate is provided to improve a leaching yield and to reduce a leaching time of uranium by adding iron sulfate. CONSTITUTION: A high efficient sulfuric acid leaching method of uranium ore by addition ferric sulfate comprises follows. The uranium is leached by adding water, sulfuric acid, oxidizer, iron sulfate to the mineral containing uranium. PH is controlled to be within 1~2 in the leaching reaction. The oxidation-reduction reaction is controlled to 400~550mV(120). PH is controlled by the input of the sulfuric acid in the leaching reaction. The oxidation-reduction reaction is controlled by the input amount of oxidizer. The iron sulfate is added by 0.1~1 parts by weight about the mineral containing uranium of 100 parts by weight. The leaching temperature is 30~60C. The mineral containing the uranium is pulverized to be particle size of 45~200 mesh. The leaching reaction is performed for 0.5~4 hours. Mixing is mixed to in 200~500rpm.
机译:目的:通过添加硫酸铁提供一种高效的铀矿硫酸浸出方法,以提高浸出率,并通过添加硫酸铁来减少铀的浸出时间。组成:一种通过添加硫酸铁对铀矿石进行高效硫酸浸出的方法,包括以下方法。通过将水,硫酸,氧化剂,硫酸铁添加到含铀的矿物中来浸出铀。在浸出反应中,PH值控制在1〜2以内。氧化还原反应控制在400〜550mV(120)。 PH由浸出反应中硫酸的输入控制。氧化还原反应由氧化剂的输入量控制。相对于100重量份的含铀矿物,添加0.1〜1重量份的硫酸铁。浸出温度为30〜60℃。将含铀的矿物粉碎成45〜200目粒度。浸出反应进行0.5〜4小时。混合以200〜500rpm的速度搅拌。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号