Method for multi-step reduction of low grade nickel ore and concentration method in nickel recovery from low grade nickel ore using the same

机译:低品位镍矿的多步还原方法及利用该方法从低品位镍矿中回收镍的浓缩方法

摘要

The present invention relates to a multistage reduction method for a low-grade nickel ore and a method for concentrating and recovering nickel using the same, and more particularly, to a method for reducing nickel-containing raw material using a gas containing CO as a reducing gas, And a second reducing step of reducing the nickel-iron-containing raw material to hydrogen gas to produce a reducing raw material for leaching, wherein the multi-step reduction method of the low grade nickel ore; And a method for efficiently concentrating and recovering nickel, including the same. The multi-step reduction method of the present invention uses a gas containing CO and a hydrogen gas to perform a two-stage reduction step. Further, the hydrogen is supplied to the process cost So that an efficient process can be performed. According to the present invention, since the reducing process is performed in multiple stages, it is possible to reduce the variation of the reducing raw material due to unevenness of the raw material quality by controlling the two-step process.
机译:低品位镍矿的多级还原方法及使用该方法进行精矿和回收镍的方法技术领域本发明涉及一种低品位镍矿的多级还原方法及使用该方法精矿和回收镍的方法,更具体地,涉及一种使用含CO的气体作为还原剂还原含镍原料的方法。第二步,将含镍铁的原料还原为氢气,制成用于浸出的还原原料。以及一种有效地浓缩和回收镍的方法。本发明的多步还原方法使用包含CO和氢气的气体来进行两步还原步骤。此外,将氢气供应至处理成本,从而可以执行有效的处理。根据本发明,由于还原处理是分多个阶段进行的,因此通过控制两步处理,能够减少由于原料品质的不均引起的还原原料的偏差。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号