The present invention relates to an environmentally-friendly marine concrete composition and a construction method using the same. According to the present invention, the environmentally-friendly marine concrete composition comprises, with respect to 100 parts by weight of seaweed: 20 to 150 parts by weight of cement; 10 to 1,000 parts by weight of aggregates; 5 to 20 parts by weight of charcoal powder; 10 to 40 parts by weight of calcium sulfoaluminate; 3 to 15 parts by weight of methyl(meta)acrylate; 2 to 10 parts by weight of metakaolin; 20 to 60 parts by weight of blast furnace slag; 10 to 70 parts by weight of fly ash; 0.01 to 5 parts by weight of a curing promoter; 0.5 to 5 parts by weight of a deformer; and 0.01 to 5 parts by weight of a high performance water reducer. According to the present invention, the environmentally-friendly marine concrete composition, which uses seaweed to stably perform ultraviolet ray absorption and air purification by absorbing carbon dioxide included in the air, reduce marine pollution, such as microplastic and the like, and increase durability, prevents damage including deterioration, erosion, and breakage caused by wave, spray, wind, and the like in and on the sea, minimizes generation of fine materials generated from marine concrete and microplastic, which is a binder of concrete, and increases strength, reduces a crack, and increases rebar corrosion resistance, freezing-thawing resistance, salinity infiltration resistance, and the like, thereby providing an effect of increasing durability.
机译:本发明涉及一种环境友好的海洋混凝土组合物及其使用方法。根据本发明,该环保型海洋混凝土组合物包含相对于100重量份的海藻:20至150重量份的水泥;和相对于100重量份的海藻。骨料10至1000重量份; 5至20重量份的木炭粉; 10至40重量份的硫铝酸钙; 3至15重量份的(甲基)丙烯酸甲酯; 2至10重量份偏高岭土; 20至60重量份的高炉矿渣; 10至70重量份的粉煤灰; 0.01-5重量份的固化促进剂; 0.5至5重量份的变形器;和0.01至5重量份的高性能减水剂。根据本发明,使用海藻通过吸收空气中所含的二氧化碳来稳定地进行紫外线吸收和空气净化,减少海洋污染物如微塑性等并提高耐久性的海藻混凝土环保组合物,防止由于海中和海上的波浪,喷雾,风等引起的损坏(包括变质,腐蚀和破裂),最大程度地减少了作为混凝土粘合剂的海洋混凝土和微塑性塑料产生的精细材料的产生,并提高了强度,降低了裂纹,并且提高了钢筋的耐腐蚀性,耐冻融性,耐盐度渗透性等,从而提供了提高耐久性的效果。

著录项

  • 公开/公告号KR102079643B1

    专利类型

  • 公开/公告日2020-02-21

    原文格式PDF

  • 申请/专利号KR20190175941

  • 发明设计人 LEE PYUNGWON;KANG CHANG GU;

    申请日2019-12-27

  • 分类号C04B24/38;C04B14/10;C04B18/08;C04B18/10;C04B18/14;C04B24/26;C04B28/06;E02B15;C04B103/14;C04B103/30;C04B103/50;