摘要

The present invention relates to a cement mortar composition having excellent constructability and waterproofness, and a repair method for a concrete structure, an injection repair method for a concrete structure, a surface treatment method for a concrete structure, and a surface protection treatment method for a concrete structure using the cement mortar composition. The cement mortar composition is composed of: 15-55 wt% of a cement-based binder; 15-55 wt% of fine aggregate; 0.1-30 wt% of a polymer-based admixture; and 5-40 wt% of water. The cement-based binder is composed of: 20-80 wt% of particle cement having 3,500-7,000 cm^2/g of Blaine fineness; 5-35 wt% of plaster; 10-40 wt% of calcium aluminate, and 0.1-10 wt% of lithium carbonate. The polymer-based admixture is composed of: 45-85 wt% of a polyurethane resin; 0.1-25 wt% of an isocyanate-based curing agent; 0.1-20 wt% of dibutyltin dilaurate; and 0.01-15 wt% of phosphazene. Therefore, the cement mortar composition can be easily constructed in a short time by being cured quickly, and can have excellent waterproofness and durability.
机译:本发明涉及具有优异的施工性和防水性的水泥砂浆组合物,混凝土结构的修复方法,混凝土结构的注射修复方法,混凝土结构的表面处理方法和用于混凝土的表面保护处理方法。混凝土结构采用水泥砂浆组成。该水泥砂浆组合物包含:15-55重量%的水泥基粘合剂;和细骨料的15-55 wt%; 0.1-30 wt%的聚合物基混合物;和5-40重量%的水。该水泥基粘合剂由以下组成:20-80wt%的具有3,500-7,000cm 2 / g的布莱恩细度的颗粒水泥;和石膏的5-35 wt%; 10-40重量%的铝酸钙和0.1-10重量%的碳酸锂。聚合物基混合物由以下组成:45-85 wt%的聚氨酯树脂; 0.1-25 wt%的基于异氰酸酯的固化剂; 0.1-20重量%的二月桂酸二丁基锡;和0.01-15wt%的磷腈。因此,水泥砂浆组合物可以通过快速固化而在短时间内容易地构造,并且可以具有优异的防水性和耐久性。

著录项

  • 公开/公告号KR102088407B1

    专利类型

  • 公开/公告日2020-03-13

    原文格式PDF

  • 申请/专利权人 BAEK SUNG JIN;

    申请/专利号KR20190051285

  • 发明设计人 BAEK SUNG JIN;KIM NAM SEOB;

    申请日2019-05-02

  • 分类号C04B28/14;C04B16/02;C04B18/14;C04B22/10;C04B24;C04B24/02;C04B24/16;C04B24/28;C04B41/52;C04B7/32;E04G23/02;

  • 国家 KR

  • 入库时间 2022-08-21 11:05:09

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号