In this study, the feasibility of using municipal solid waste incineration fly ash (MSWIFA) as additive for the strengthening of pretreated cement-stabilized soil was evaluated. Results indicated that the leaching concentrations of chromium and lead in MSWIFA after the water washing process and addition of 4% ferrous sulphate were reduced by 67% and 89%, respectively, which was lower than the limit value of Identification standard for hazardous waste (GB 5085.3-2007). After pretreatment, MSWIFA samples with ratios of 5% and 10% were blended into cement-stabilized soil with ordinary Portland cement (OPC) content of 10%, 15% and 20%. The unconfined compressive strength (UCS), internal friction angle and cohesion of the cement-stabilized soil increased with OPC and pretreated MSWIFA (PFA) content. The same effect was observed on UCS after the addition of 10% PFA as replacement of 5% OPC. In the subsequent X-ray powder diffraction test, scanning electron microscopy and leaching tests, the leaching concentrations of heavy metals in cement-stabilized soil became far lower than the limit value under the synergis-tic effects of the physical encapsulation of hydration products and stabilization of chemical agents. The incorporation of PFA as a supplementary material can effectively accelerate the formation of hydration products and can thus provide cleaner options for foundation reinforcement.
机译:在这项研究中,评估了使用城市固体废物焚烧粉煤灰(Mswifa)作为加强预处理水泥稳定土壤的添加剂的可行性。结果表明,水洗过程后,铬酸铬和铅的浸出浓度分别减少了67%和89%,低于危险废物鉴定标准的限值(GB 5085.3-2007)。在预处理后,具有5%和10%的比率的Mswifa样品与普通植物水泥(OPC)含量为10%,15%和20%的水泥稳定的土壤。使用OPC和预处理的MswifA(PFA)含量增加了无凝结的压缩强度(UCS),内部摩擦角和水泥稳定的土壤的内聚力。在加入10%PFA后,在UCS中观察到相同的效果作为替换5%OPC。在随后的X射线粉末衍射试验中,扫描电子显微镜和浸出试验中,水泥稳定土壤中重金属的浸出浓度变得远低于水合产物物理封装和稳定化的协同效应下的极限值。化学试剂。作为补充材料的PFA掺入可以有效地加速水合产物的形成,因此可以为基础加固提供清洁选项。

著录项

  • 来源
    《Waste Management》 |2020年第3期|425-432|共8页
  • 作者单位

    School of Civil and Transportation Engineering Guangdong University of Technology No. 100 Waihuan Xi Road Guangzhou 510006 China;

    School of Civil and Transportation Engineering Guangdong University of Technology No. 100 Waihuan Xi Road Guangzhou 510006 China;

    School of Civil and Transportation Engineering Guangdong University of Technology No. 100 Waihuan Xi Road Guangzhou 510006 China;

    School of Civil and Transportation Engineering Guangdong University of Technology No. 100 Waihuan Xi Road Guangzhou 510006 China;

    Dongguan Institute of Building Research Lianma Road Dongguan 523820 China;

    Guangzhou Environmental Protection Investment Crouv Co.. Ltd. No. 1226 Xineanz East Road. Guanzzhou 510330 China;

  • 收录信息
  • 原文格式 PDF
  • 正文语种 eng
  • 中图分类
  • 关键词

    MSWIFA; Pretreatment; Cement-stabilized soil; Synergistic effect; Unconfined compressive strength;

    机译:Mswifa;预处理;水泥稳定的土壤;协同效应;无束缚的抗压强度;

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号