Synthesis and characterization of platinum nano sized particles by laser ablation in C_2H_6O_2 solution

机译:在C_2H_6O_2溶液中激光烧蚀制备纳米铂纳米粒子及其表征。

获取原文
获取原文并翻译 | 示例
           

摘要

Platinum nano sized particles (Pt NPs) are superior catalysts for many intentions, such as glucose sensors, cancer therapy, gas sensors, etc. Here, Pt NPs were produced by pulsed laser ablation in C_2H_6O_2 solution using Q-switched Nd:YAG laser, for the first time. Then, the influence of the laser fluence during synthesis of them was investigated; and they were characterized by UV-vis spectroscopy, TEM, FE-SEM, XRD, FT-IR, and Raman spectroscopy. The results showed that with increasing laser fluence, the mean particle size of the spherical NPs enhanced. Meanwhile, they had a polycrystalline cubic structure. Correspondingly, the plasmon peak position of generated NPs in the absorption spectra shifted from 257 to 266 nm, with a rise of laser fluence. The IR and Raman spectroscopy was used to achieve the information about the surface state of Pt NPs. We propose that the optimum adjusted laser fluence is an important factor to increase the ablation efficiency.
机译:铂纳米颗粒(Pt NPs)是许多目的的优良催化剂,例如葡萄糖传感器,癌症治疗,气体传感器等。这里,Pt NPs是通过使用Q开关Nd:YAG激光在C_2H_6O_2溶液中通过脉冲激光烧蚀产生的,首次。然后研究了激光能量密度在合成过程中的影响。并通过紫外可见光谱,TEM,FE-SEM,XRD,FT-IR和拉曼光谱进行了表征。结果表明,随着激光通量的增加,球形NP的平均粒径增加。同时,它们具有多晶立方结构。相应地,随着激光通量的增加,在吸收光谱中产生的NP的等离子体激元峰位置从257nm移至266nm。红外光谱和拉曼光谱用于获得有关Pt NPs表面状态的信息。我们建议最佳的调整激光能量密度是增加烧蚀效率的重要因素。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号