Synthesis of a two-phase nanopowder from prototype human synovial fluid and the use of the nanopowder for the preparation of coatings on titanium plates

机译:由原型人体滑液合成两相纳米粉末及其在钛板上制备涂层的应用

获取原文
获取原文并翻译 | 示例
   

获取外文期刊封面封底 >>

       

摘要

Using prototype human synovial fluid, we have synthesized a calcium phosphate nanopowder consisting of two crystalline phases (whitlockite and carbonate-containing hydroxyapatite). The nanopowder was used to produce calcium phosphate (monetite) coatings on titanium substrates by microarc oxidation. It has been shown that, with increasing microarc oxidation voltage (from 200 to 300 V), the mass, thickness, roughness parameter, and Ca : P ratio of the coatings increase linearly. Increasing the voltage to 300 V and the calcium phosphate coating growth time to 10 min allows a single-phase coating up to 100 mu m in thickness, consisting of monetite nanocrystals, to be produced on a metallic surface and its adhesion strength to be improved.
机译:使用原型人体滑液,我们合成了由两个晶相(硅钙石和含碳酸盐的羟基磷灰石)组成的磷酸钙纳米粉。纳米粉被用于通过微弧氧化在钛基底上生产磷酸钙(蒙脱石)涂层。已经表明,随着微弧氧化电压的增加(从200到300 V),涂层的质量,厚度,粗糙度参数和Ca:P比呈线性增加。将电压提高到300 V,将磷酸钙涂层的生长时间提高到10分钟,可以在金属表面上生产厚度最大为100μm的单晶涂层,该涂层由褐铁矿纳米晶体组成,并且可以提高其粘合强度。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号