Chitosan stabilized silver nanoparticles (AgNPs) were synthesized using gamma ray irradiation. Four different sample solutions were prepared [1 mM AgNO3 in 0.1% (w/v) chitosan, 1 mM AgNO3 in 0.5% (w/v) chitosan, 2 mM AgNO3 in 0.1% (w/v) chitosan 2 mM AgNO3 in 0.5% (w/v) chitosan] with controls maintaining dose of radiation at 20±2 kGy. The formation of AgNPs were determined by the appearance of the characteristic colour of the AgNPs, using the surface plasmon resonance band (SPR) at 400-432 nm range and the N-H band of the FT-IR spectrum. Stability of the maximum absorption wave lengths of the samples was monitored for three months by UV-visible spectroscopy. The particle size distribution of the stabilized sample, showed a wide distribution of 28-1106 nm. The sample, 2 mM AgNO3 in 0.5% (w/v) chitosan was stable for three months. FT-IR spectroscopic analysis revealed a shifting of N-H stretching vibration band from 3367-3228 cm-1 with the introduction of nanoparticles.
机译:壳聚糖稳定的银纳米粒子(AgNPs)使用伽玛射线辐射合成。制备了四种不同的样品溶液[含0.1%(w / v)壳聚糖的1 mM AgNO3,含0.5%(w / v)壳聚糖的1 mM AgNO3,含0.1%(w / v)壳聚糖的2 mM AgNO3,含0.5%壳聚糖的2 mM AgNO3 [%(w / v)壳聚糖]与对照将辐射剂量维持在20±2 kGy。使用在400-432 nm范围内的表面等离振子共振带(SPR)和FT-IR光谱的N-H谱带,通过AgNPs的特征颜色的出现来确定AgNPs的形成。通过紫外-可见光谱法监测样品的最大吸收波长的稳定性三个月。稳定样品的粒度分布显示出28-1106 nm的宽分布。样品,含0.5%(w / v)壳聚糖的2 mM AgNO3稳定了三个月。 FT-IR光谱分析表明,随着纳米颗粒的引入,N-H拉伸振动带从3367-3228 cm-1发生了位移。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号