Recovering Y and Eu from waste phosphors using chlorination roasting followed by a water leaching process was investigated in this study. Firstly, by chlorination roasting and water leaching, Y and Eu elements present in waste phosphors were efficiently extracted into a leach solution. Secondly, the majority of the impurities in the solution can be removed by adjusting the pH to 4.5 using a Na 2 S and NH 3 ???·H 2 O solution. Thirdly, the rare earths can be precipitated afterwards by adding a H 2 C 2 O 4 solution and adjusting the pH to 2.0. Then rare earth oxides (REOs) can be obtained after calcining at 800 ???°C for 1 h. The characterization study of the waste phosphors and the rare earth oxide products was performed by XRD, XRF, and SEM-EDS analysis to determine the phase and morphological features. Influences of the factors, such as roasting temperatures and time, the addition of ammonium chloride on the roasting of waste phosphors, as well as the pH and the amount of oxalates on the precipitation of Y and Eu, were investigated. The maximum grade (99.84%) of mixed rare earth oxides and recovery rate (87.35%) of Y and Eu were obtained at the optimized conditions.
机译:本研究研究了采用氯化焙烧和水浸工艺从废磷中回收Y和Eu。首先,通过氯化焙烧和水浸,废磷中存在的Y和Eu元素被有效地萃取到浸出溶液中。其次,可以通过使用Na 2 S和NH 3·H 2 O溶液将pH调节至4.5来除去溶液中的大部分杂质。第三,随后可以通过添加H 2 C 2 O 4溶液并将pH值调节到2.0来沉淀稀土。然后在800℃下煅烧1小时后可获得稀土氧化物(REOs)。通过XRD,XRF和SEM-EDS分析对废荧光粉和稀土氧化物产物进行表征研究,以确定其相态和形态特征。研究了焙烧温度和时间,氯化铵的添加对废磷的焙烧以及pH值和草酸盐含量对Y和Eu沉淀的影响。在最佳条件下,获得了稀土混合氧化物的最高品位(99.84%)和Y和Eu的回收率(87.35%)。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号