Experimental Evaluation of Efficient Si Dissolution from Perlite at Low Level Activator’s Concentration

机译:低浓度活化剂对珍珠岩有效溶解硅的实验评估

获取原文
           

摘要

This paper deals with the Si dissolution of fine perlite in alkaline solutions for the determination of the SiO 2 /Na 2 O mass ratio in the aqueous phase of geopolymer slurries. In the present work, the effect of the main synthesis parameters such as NaOH concentration and curing temperature on the setting time of the paste were studied. The obtained results showed that the inorganic polymer pastes present fast hardening at low concentrations of NaOH solutions for both 70 and 90 ° C. This observation was also identified by the Si dissolution study of perlite pastes as a function of different concentrations of NaOH solutions and different solid to liquid ratios of the slurries, under a constant temperature. The optimum synthesis conditions for geopolymer pastes proved to be a low initial NaOH concentration in the alkaline phase (2–4 M NaOH), where the fast hardening of the paste was attributed to the high SiO 2 /Na 2 O mass ratio, enhancing the polycondensation phenomena and promoting the geopolymerization process.
机译:为了确定地质聚合物浆料水相中SiO 2 / Na 2 O的质量比,本文研究了细珍珠岩在碱性溶液中的Si溶解。在本工作中,研究了主要合成参数(如NaOH浓度和固化温度)对糊剂凝固时间的影响。所得结果表明,无机聚合物浆料在低浓度的NaOH溶液中分别在70和90°C时呈现快速硬化。这一观察结果也通过珍珠岩浆料的Si溶出度研究确定为不同浓度的NaOH溶液和不同的NaOH溶液的函数。在恒定温度下,浆液的固液比。事实证明,地质聚合物浆料的最佳合成条件是在碱相中的初始NaOH浓度较低(2-4 M NaOH),其中浆料的快速硬化归因于较高的SiO 2 / Na 2 O质量比,从而提高了缩聚现象,促进了地聚过程。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号