Economic and environmental considerations have encouraged the incorporation of Reclaimed Asphalt Pavement (RAP) in the new asphalt mixtures. The Stone Mastic Asphalt (SMA) mixture is a gap-graded mixture, which performs better than the conventional dense-graded mixtures. To incorporate RAP into SMA mixtures certain setbacks are to be mitigated. RAP consists of aged binder, which is aged due to oxidation. Because of ageing process, this binder will have a higher stiffness than that of the virgin binder. A rejuvenator is included to decrease the stiffness and that permits high RAP content. In this study, Waste Engine Oil (WEO) and Waste Grease (WG) are used as rejuvenators. The RAP content is varied at four levels (10, 20, 30 and 40% by weight of the aggregate) and at each level rejuvenator's dosage is varied at 0, 3, 6 and 9% (by weight of the asphalt). Overall, 29 SMA mixture combinations are considered and laboratory-scale performances are studied. The statistical analysis such as three-way Analysis of Variance (ANOVA) test and main effect plot are performed to evaluate the significance of the three independent variables (i.e. RAP content, rejuvenator type and dosages) on the response variables (i.e. optimum binder content, Marshall quotient, retained Marshall stability and tensile strength ratio). From the results, it is concluded that 40% RAP content SMA mixtures can be produced without compromising the stone-on-stone contact, volumetric properties and moisture resistance. The statistical analysis points out that the WEO performed better than the WG. Overall, it is determined that 30% RAP with 6% WEO is superior SMA mixture with better performance. (C) 2020 Elsevier Ltd. All rights reserved.
机译:经济和环境考虑鼓励在新的沥青混合物中加入回收沥青路面(RAP)。石棉沥青(SMA)混合物是间隙分级混合物,其比传统的致密集混合物更好。将RAP掺入SMA混合物混合中应减轻某些挫折。 RAP由老年粘合剂组成,这是由于氧化而老化的。由于衰老过程,该粘合剂具有比原始粘合剂更高的刚度。包括恢复剂以减少刚度并允许高的RAP含量。在本研究中,废物发动机油(WEO)和废物油脂(WG)用作再融化器。 RAP含量在四个水平(10,20,30和40重量%的聚集体中)而变化,并且在每个级别的雷化剂的剂量在0,3,6和9%(重量的沥青的重量)中变化。总体而言,考虑了29个SMA混合混合物组合,研究了实验室级性能。进行统计分析,例如差异的三元分析(ANOVA)测试和主要效果图,以评估三个独立变量(即RAP含量,再血清类型和剂量)对响应变量的意义(即最佳粘合剂含量,马歇尔商量,保留马歇尔稳定性和拉伸强度比)。从结果中,得出结论,可以生产40%的RAP含量SMA混合物,而不会影响石头接触,体积性能和防潮性。统计分析指出,WEO比WG更好。总体而言,确定30%的Hyp具有6%Weo的RAP是具有更好性能的优质SMA混合物。 (c)2020 elestvier有限公司保留所有权利。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号