The aim of this study is to investigate the silver recovery from aqueous solutions. There are a variety of recovery methods, such as hydrometallurgical, bio-metallurgical, cementation, reduction, electrocoagulation, electrodialysis, ion exchange, etc. Adsorption represents a convenient, environment friendly procedure, that can be used to recover silver from aqueous solutions. In this paper we highlight the silver adsorption mechanism on chitosan chemically modified with active groups, through kinetic, thermodynamic, and equilibrium studies. A maximum adsorption capacity of 103.6 mg Ag(I)/g of adsorbent for an initial concentration of 700 mg/L was noticed by using modified chitosan. Lower adsorption capacity has been noticed in unmodified chitosan—a maximum of 75.43 mg Ag(I)/g. Optimum contact time was 120 min and the process had a maximum efficiency when conducted at pH higher than 6. At the same time, a way is presented to obtain metallic silver from the adsorbent materials used for the recovery of the silver from aqueous solutions.
机译:这项研究的目的是研究从水溶液中回收银。有多种回收方法,例如湿法冶金,生物​​冶金,胶结,还原,电凝,电渗析,离子交换等。吸附是一种方便,环保的方法,可用于从水溶液中回收银。在本文中,我们通过动力学,热力学和平衡研究重点介绍了用活性基团化学修饰的壳聚糖对银的吸附机理。通过使用改性壳聚糖,初始浓度为700 mg / L时,吸附剂的最大吸附容量为103.6 mg Ag(I)/ g。在未改性的壳聚糖中,吸附能力较低,最大吸附量为75.43 mg Ag(I)/ g。最佳接触时间为120分钟,在pH值高于6的条件下进行时,该工艺具有最高效率。同时,提出了一种从用于从水溶液中回收银的吸附剂材料中获得金属银的方法。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
代理获取

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号