Mg65Ni10RE25(RE=La,Ce,Pr,Nd,Mm)非晶储氢合金电极的性能

         

摘要

The amorphous Mg 65 Ni 10 RE 25 alloys were prepared by copper-mold injection casting, and the structure, corrosion resistance property and discharge capacity of Mg65Ni10RE25 alloys were investigated by using XRD, electrical chemical test and discharge capacity test. The structure and chemical stability of the amorphous Mg 65 Ni 10 RE 25 alloys were also evaluated by the parameters related to the glass-forming ability. The results show that the Mg 65 Ni 10 La 25 , Mg65Ni10Nd25 and Mg65Ni10Mm25 alloys all have an amorphous structure. Moreover, due to the addition of rare earth elements, the glasses-forming ability of Mg65Ni10Mm25 will be improved, and the crystallization will be inhibited. The addition of rare earth elements can accelerate the reaction rate, which becomes the main reason for the degradation of the discharge capacity.%通过XRD、动电位极化法和放电容量测试等手段对Mg 65 Ni 10 RE 25的非晶合金电极结构、耐腐蚀性和放电容量等性能进行了分析,并采用表征非晶合金形成能力的参数对其结构和化学稳定性进行了评价。结果表明:设计的Mg 65 Ni 10 La 25、Mg 65 Ni 10 Nd 25和Mg 65 Ni 10 Mm 25具有典型的非晶结构特征。其中,Mg 65 Ni 10 Mm 25通过增加组元提高了非晶合金的形成能力,同时,较高的原子堆垛密度和强烈的原子间相互作用抑制了晶化的进行,使其具有良好的稳定性;但多组元的添加则加速了合金在溶液中的腐蚀反应,是导致Mg 65 Ni 10 Mm 25非晶储氢合金电极放电容量降低的主要原因。

著录项

相似文献

  • 中文文献
  • 外文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号