CHROME-MAGNESITE REFRACTORY CORROSION WITH OLIVINE SLAG OF HIGH CUPROUS OXIDE CONTENT

机译:氧化铜含量高的橄榄石渣对铬镁矿的耐蚀性

获取原文
获取原文并翻译 | 示例

摘要

Continuous converting of copper matte produces slag with high cuprous oxide content. The corrosion of chrome-magnesite refractories with slag of high cuprous oxide content is a major problem. Properties of olivine type of slag make the slag very attractive for matte smelting and converting. Analysis of phenomena determining the slag infiltration into the porosity of a refractory and dissolution of refractory components in the slag allowed for better understanding of the mechanisms of refractory destruction. The results of laboratory scale tests of the olivine slag infiltration into open porosity and corrosion showed dominating effects of slag temperature and cuprous oxide content. The optical and X-ray examination of slag samples permitted the definition of the mechanism of formation of new phases and refractory deterioration.
机译:铜mat的连续转化会产生高氧化亚铜含量的炉渣。高氧化亚铜含量的炉渣对铬-镁砂质耐火材料的腐蚀是一个主要问题。橄榄石型炉渣的性质使该炉渣对于毛面熔炼和转化非常有吸引力。对确定炉渣渗入耐火材料孔隙的现象以及炉渣中耐火成分的溶解现象的分析有助于更好地理解耐火材料的破坏机理。橄榄石矿渣渗透到开放孔隙和腐蚀中的实验室规模试验结果表明,矿渣温度和氧化亚铜含量起主要作用。炉渣样品的光学和X射线检查可以确定新相的形成和耐火材料劣化的机理。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号