A Method to Test Anterior-Posterior Construct Shear Fatigue Based on the Vertebrectomy Model

机译:基于椎骨切除术模型的前-后构建体剪切疲劳测试方法

获取原文
获取原文并翻译 | 示例

摘要

Dynamic stabilization systems may be subject to anterior-posterior shear loading. However, there is no standard method established for testing a vertebrectomy model in anterior-posterior translation (as may be seen with dynamic spondylolisthesis). A new anterior-posterior shear fatigue test was devised to test one such dynamic stabilization system in anterior-posterior translation. Similar to ASTMF1717 assemblies, constructs were assembled so that screws were placed in ultra high molecular weight polyethylene blocks to attach to the test fixture. The test setup ensures that the entire shear load is transmitted by the implant system. Unlike ASTMF1717 assemblies, the blocks were rotated 180 deg from each other to facilitate loading in the test frame. This configuration is modified from an expected in vivo usage. However, the resultant load vectors are appropriately similar to the shear loads being simulated. The constructs include polymeric components and thus were tested at body temperature in a fluid bath. The blocks were moved ±5 mm with respect to each other. The constructs were cycled at 2 Hz for a minimum of 5 × 10~6 cycles. The constructs successfully survived 10 × 10~6 cycles of anterior-posterior shear displacement. Examination of the constructs demonstrated similarities between components tested via this new method and components retrieved from patients. Comparisons indicate that the shear fatigue test may stress the components as much or perhaps more than what was seen clinically.
机译:动态稳定系统可能会经受前后剪切荷载。但是,目前尚无用于测试椎骨切除术模型前后平移的标准方法(如动态脊椎滑脱所见)。设计了一种新的前后剪切疲劳试验,以测试这样一种动态稳定系统的前后位移。与ASTMF1717组件类似,将结构组装在一起,以便将螺钉放置在超高分子量聚乙烯块中以连接到测试夹具。测试设置可确保整个剪切负荷均由植入系统传递。与ASTMF1717组件不同,模块彼此旋转了180度,以方便在测试框架中加载。根据预期的体内用法修改了此配置。但是,所得载荷矢量与模拟的剪切载荷适当相似。该构建体包括聚合物组分,因此在体温下在流化浴中进行测试。这些块相对于彼此移动±5mm。将构建体以2 Hz的频率循环至少5×10〜6个循环。该结构成功地经受了前后剪切位移的10×10〜6个循环。对构建体的检查表明,通过这种新方法测试的组件与从患者身上检索到的组件之间具有相似性。比较表明,剪切疲劳试验对部件的应力可能大于或大于临床所见。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号