The reduced blastfurnace titanium slag, made in Panzhihua Steel and Iron Corporation, contains a lot of minerals with low melting temperature, such as C_2AS, CS, CMS_2-CTS, etc.. It can be used as the raw materials fully or partly replacing clay to produce cement clinker. These minerals in the reduced slag are benefit to accelerate the formation of clinker minerals by reducing the eutectic temperature. The sintering temperature of clinker is about 1350 degree when the reduced titanium slag is added in the raw mixes. The cement strength may reach 525# level when as high as 20
机译:攀枝花钢铁公司生产的还原高炉钛渣含有很多熔融温度低的矿物,例如C_2AS,CS,CMS_2-CTS等。它可以完全或部分代替粘土用作原料。生产水泥熟料。降低炉渣中的这些矿物通过降低共晶温度有利于加速熟料矿物的形成。当将还原的钛渣添加到原始混合物中时,熟料的烧结温度为约1350度。水泥强度高达20时可达到525#

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号